对江汉平原水杉、池杉、落羽杉人工林物理力学性能进行了研究,结果表明:落羽杉的密度和硬度最大;落羽杉、水杉、池杉的抗弯强度差异不大;水杉的弹性模量最大,约为落羽杉的2.3倍,落羽杉的弹性模量与池杉的比较接近。南北方向对水杉、池杉、落羽杉的密度、顺纹抗压强度在5%水平上差异均不显著,对池杉、水杉抗弯强度在5%水平上差异不显著,对落羽杉抗弯强度在1%水平上差异显著,对落羽杉、池杉的弹性模量在1%水平上差异显著,对水杉的弹性模量在5%水平上差异不显著。三杉南北面近树皮处木材的密度、抗弯强度、弹性模量、顺纹抗压强度均大于髓心处。对水杉、池杉、落羽杉物理力学性能比较研究,旨在为其培育及合理利用提供依据。  相似文献   

2.
参照国家标准,对我国木材市场典型的进口针叶树木材——辐射松进行物理性能和力学性能的研究。结果表明,辐射松木材气干密度较低,径向干缩率与湿胀率均小于弦向,径向尺寸稳定性优于弦向;端面硬度弦面硬度径面硬度;抗弯强度等级为中,弹性模量、顺纹抗剪强度、顺纹抗压强度、冲击韧性等级为低。在实际应用时需充分考虑其材质特点,适材适用。  相似文献   

3.
本研究对田间试验林中8年生转基因741杨与非转基因741杨木材物理力学性质进行了对比分析。结果表明,转基因741杨的横纹抗压比例极限应力除了全部弦向略低于非转基因741杨外,干缩性、抗弯强度、顺纹抗压强度转基因741杨均高于非转基因741杨。除了干缩性差异不显著外,大部分性质差异显著,均达0.01极显著水平。抗弯强度、抗弯弹性模量、顺纹抗压强度和木材横纹全部径向抗压极限应力差异达0.01极显著水平。绝干密度、弦面握钉力和冲击韧性差异达0.05显著水平。其余性质的差异并不显著。  相似文献   

4.
人工林杉木和杨树木材物理力学性质的株内变异研究   总被引:4,自引:0,他引:4  
按照中国国家标准研究杉木和I-214杨树木材的抗弯弹性模量、抗弯强度、顺纹抗压强度和密度,同时按照日本国家标准研究2个树种的顺纹抗剪强度.结果表明:杉木的抗弯强度、顺纹抗压强度和密度由胸高直径处向上呈波浪形增加,抗弯弹性模量则稳定降低,但不同高度间杉木的物理力学性质没有显著差异;近树皮处木材的物理力学性质高于近髓心处木材,并有极显著差异.对于I-214杨树,只有抗弯弹性模量从髓心到树皮逐渐增加,其他的物理力学性质,最小值在从髓心到树皮的过渡区,最大值在近树皮处,从髓心到树皮,杨树的物理力学性质有极显著的差异.杉木和杨树的径面顺纹抗剪强度从髓心到树皮有极显著差异,并且近树皮的高于近髓心的木材,而弦面顺纹抗剪强度从髓心到树皮没有显著差异.木材密度与力学性质有很好的线性相关关系,木材密度是一个很好的力学强度的预测手段.  相似文献   

5.
湿地松与马尾松人工林木材物理力学性质的比较研究   总被引:2,自引:0,他引:2  
通过对湿地松和马尾松人工林木材物理力学性质的测定和比较分析,结果表明:湿地松人工林木材密度、干缩系数和除冲击韧性以外的力学强度均稍大于马尾松人工林木材,而冲击韧性则恰恰相反.经差异显著性t检验表明:湿地松和马尾松木材物理力学性质指标中顺纹抗压强度、抗弯强度、弦面顺纹抗剪强度和冲击韧性差异极显著,气干密度、基本密度、径面顺纹抗剪强度和端面硬度差异显著,除此之外的其余指标差异不显著.  相似文献   

6.
间伐强度对湿地松木材性质的影响规律研究   总被引:5,自引:1,他引:5       下载免费PDF全文
通过对不同间伐强度处理 (未间伐、弱度 (伐去株数 18 6 % )、中度 (伐去 35 7% )、强度 (伐去5 2 9% ) )的 19年生湿地松林分其林木木材的主要材性指标进行全面测试分析研究 ,结果表明 :间伐后 8a ,间伐强度对湿地松木材气干密度、全干密度、径向全干缩率、体积全干缩率、差异干缩、顺纹抗压强度、抗弯强度、弹性模量、径向抗剪强度及端面硬度有显著影响 ;随着间伐强度的增大 ,树干年生长轮平均宽度、木材差异干缩是增大的 ,而随间伐强度的增加木材气干密度、全干密度有不同程度的减小 ,木材顺纹抗压强度、抗弯强度、抗弯弹性模量、硬度等主要力学性质则是呈先增加后减小的趋势。  相似文献   

7.
楸树新无性系木材的物理力学性质   总被引:1,自引:0,他引:1  
对采自于河南省南阳市的21年生楸树新无性系宛楸8401和宛楸8402与生产上广泛应用的金丝楸无性系进行木材主要物理力学性质的对比研究.结果表明:3个无性系的基本密度、气干密度、端面硬度、弦面硬度、径面硬度、抗弯强度、抗弯弹性模量、顺纹抗压强度、顺纹抗拉强度、冲击韧性、弦向抗剪强度和径向抗剪强度差异极显著,宛楸8401和金丝楸相近,且显著优于宛楸8402;3个无性系的成熟材与幼龄材的物理力学性质也表现出显著差异;与黄菠萝、核桃楸、红椿和香樟相比,宛楸8401和金丝楸与香樟和黄菠萝相近,优于红椿,但是比核桃楸稍差,宛楸8402与红椿相近.  相似文献   

8.
人工林米老排木材的物理力学性质   总被引:2,自引:0,他引:2  
对23年生人工林米老排木材物理力学性质进行了测定和分析.结果表明:木材气干密度、全干密度和基本密度分别为0.577 g/cm3,0.554 g/cm3,0.463 g/cm3,属中等级别.木材全干差异干缩和气干差异干缩分别为1.963和2.442,弦向和径向干缩湿胀差异较大;木材端面、弦面和径面的硬度分别为5 717.0 N,3 963.7 N和3 822.8 N,弦面和径面的抗劈力分别为16和14 N/mm,弦面和径面的顺纹抗剪强度分别为11.6 MPa和11.3 MPa,抗弯强度和抗弯弹性模量分别为132.3 MPa和13 092 MPa,冲击韧性为62.5 kJ/m2,顺纹抗压强度为48.7 MPa;木材综合品质系数为3 909×105Pa,品质系数非常高,属高等级材.  相似文献   

9.
参照国家标准要求,测试麻栎和栓皮栎木材的主要力学性能。结果表明:两种栎木的顺纹抗压强度、抗弯弹性模量、抗弯强度等级均为高,冲击韧性等级为甚高;硬度等级均为很硬,且端面弦面径面;树种间差异为麻栎木材的顺纹抗剪强度等级为高,栓皮栎木材为中。综合评价,两种栎木的力学性能均属于中高等材级别,麻栎木材的各项力学性能指标更高。  相似文献   

10.
15年生香樟人工林木材物理力学性质研究   总被引:1,自引:0,他引:1  
以15年生香樟(Cinnamomum camphora)人工林木材为研究对象,测定其物理力学性质,为其加工利用提供参考。结果表明,香樟人工林木材的气干密度、基本密度和绝干密度分别为0.51、0.41和0.48 g/cm^3,气干密度属于Ⅱ级;差异干缩属于中等,尺寸稳定性相对较差;端面硬度2909 N、弦面硬度2353 N、径面硬度2403 N,属于Ⅱ级,硬度偏小;顺纹抗压强度为33.4 MPa,属于Ⅱ级;抗弯强度为79 MPa,属于Ⅱ级;抗弯弹性模量为1.25 GPa,属于Ⅲ级,弹性相对较好;冲击韧性为53 kJ/m^2,属于中等;综合强度为112.4 MPa,属于中等;品质系数为274 MPa,品质系数高。  相似文献   

11.
人工林杉木木材力学性质对高温热处理条件变化的响应   总被引:6,自引:0,他引:6  
以人工林杉木为试材,分别用空气和菜子油为介质,在温度为180,200和220 ℃对其分别热处理1,3和5 h,研究试材的抗弯强度(MOR)、抗弯弹性模量(MOE)、顺纹抗压强度、表面硬度对高温热处理条件变化的响应,同时对处理材的主要化学成分进行分析,用扫描电镜对处理材横切面微观结构进行观察.结果表明:人工林杉木试材的4种主要力学性质对不同条件热处理的响应程度不同.无论是空气热处理还是油热处理,试材的MOR,MOE,顺纹抗压强度与对照比有不同程度的降低,且随处理温度升高、时间延长,下降幅度增大,相比于时间,温度的影响更显著;180 ℃热处理1,3和5 h时,试材的MOR,MOE与对照比未发生明显变化(降幅在3%以内),而顺纹抗压强度则明显低于对照,两介质中降低幅度分别在3.29%~9.58%和3.89%~7.18%;200 ℃以上处理时,不同时间处理的3种主要力学性质不仅显著或极显著低于对照,且各性质问的差异也达显著或极显著水平;对硬度的测试结果表明:180 ℃热处理时,试件的径面硬度和弦面硬度均随时间的延长而增大;200 ℃热处理3 h时,试件的硬度达最大,与对照差异达显著水平;随后热处理试件的硬度开始降低,220 ℃热处理5 h后试件的硬度又明显低于对照.在隔氧的油介质中进行热处理,4种主要力学性质的变化程度低于空气介质处理材,当温度高于200 ℃时,两介质处理间的差异达显著水平.而热处理过程中木材主要化学组成与横切面微观结构变化的差异,反映了4种主要力学性质对不同条件热处理时表现出的响应差异.  相似文献   

12.
The variation in strength properties with density was compared between semi-isostatically densified and non-densified wood. Strength properties were compared with published data from earlier studies using other methods for densification. Small clear specimens of eight species were analysed for compression strength in axial, radial and tangential direction, three-point bending and Brinell hardness. After densification, all tested strength properties increased with density, but especially strength perpendicular to grain became lower than expected from the density of non-densified wood. Strength of densified wood relative to what could be expected for non-densified wood of similar density was denoted as ‘strength potential index’. For axial compression strength and bending strength, strength potential index of individual wood species varied between 0.7 and 1.0, i.e. densified wood is slightly weaker than what could be expected from its density. Strength potential index was lower for properties much determined by strength perpendicular to grain. In radial direction, densified wood was rubbery with low modulus of elasticity and nearly no proportional limit or modulus of rupture. Generally, wood was apparently weakened in proportion to the degree of compression in respective direction. Strength potential index also increased with increasing original density of the species.  相似文献   

13.
红松幼龄材与成熟材力学性质的差异   总被引:3,自引:0,他引:3  
本文研究了人工林和天然林红松幼龄材与成熟材力学性质的差异.结果显示,成熟材的所有力学性质均高于幼龄材.幼龄材与成熟材的抗弯弹性模量差异在人工林红松中达0.01水平显著,天然林红松也达到0.01水平显著;人工林红松抗弯强度和弦向横纹抗压强度差异达0.05水平显著.抗弯强度、顺纹抗压强度、横切面硬度和弦向横纹抗压强度4项指标的差异达0.05水平显著.  相似文献   

14.
江汉平原落羽杉生长规律研究   总被引:2,自引:1,他引:1  
通过对江汉平原引种栽培的落羽杉人工林进行试验调查和树干解析,研究探讨了落羽杉树高、胸径和材积的生长规律,结果表明:落羽杉树高前期生长较快,之后逐渐减慢;胸径连年生长量和平均生长量均表现为先升后降,其中10~15 a生长最为迅速;材积生长在9 a前较慢,连年生长量在21 a达到最大,在28 a左右达到数量成熟龄,笔者对江汉平原落羽杉试验林的生长规律进行了研究,以期为落羽杉的引种栽培,造林规划和科学经营提供基础数据和理论数据。  相似文献   

15.
This study investigated the densities, average width of annual rings, and partial compression stresses at 5 % strain perpendicular to the grain of air-dried wood specimens, which were continuous in the radial direction from the pith and were obtained from Japanese larch (Larix kaempferi) trees with different diameters at breast height in the same stand, to evaluate the radial variations in partial compression properties perpendicular to the grain. The air-dried densities of the wood increased with the distance from the pith. The average width of annual rings of the wood tended to decrease with increasing distance from the pith and those of medium- and large-diameter trees seemed to increase near the pith. The partial compression stresses at 5 % strain in the tangential loading direction tended to increase with the distance from the pith and with air-dried wood density. However, in the radial loading direction, this tendency was not observed. The partial compression stresses at 5 % strain in the radial loading direction tended to be low in wood with a small average width of annual rings. These results indicate that the factors affecting the radial variations in the partial compression stress at 5 % strain differ depending on the loading directions.  相似文献   

16.
采用慈竹为原料制造竹帘胶合板,以三种不同的方式进行组坯,研究组坯方式对慈竹竹帘胶合板纵横方向静曲强度、弹性模量、压缩强度与水平剪切强度的影响。结果表明:组坯方式对胶合板的弹性模量与静曲强度影响较为显著。Ⅲ型板纵向各项力学性能最优,Ⅲ型板横向各项力学性能最弱。Ⅰ型板和Ⅱ型板的静曲强度和弹性模量均达到了汽车车厢用竹篾胶合板的A类标准。三种方式组坯板件的主要力学性能均达到了结构用竹木复合板国家A级标准与混凝土模板用胶合板主要物理力学性能指标。  相似文献   

17.
研究了不同培育措施(初植密度、间伐强度、坡向、坡位)对人工林樟子松(Pinus sylvestris var.mongolica)木材的密度和力学性质(横纹抗弯强度、抗弯弹性模量、顺纹抗压强度、冲击韧性、端面硬度)的影响。初植密度(1.5m×1.0m,1.5m×2.0m和1.5m×2.5m)对木材密度和抗弯弹性模量有显著的影响。初植密度为1.5m×1.0m时,木材主要力学指标值最大。适当间伐可提高木材的抗弯弹性模量和顺纹抗压强度,但重度间伐则会降低木材的力学强度。坡向(阳坡和阴坡)对木材的抗弯弹性模量影响显著,阳坡高于阴坡。坡位(上坡位和下坡位)对除端面硬度外的木材力学性质指标影响都显著,各项力学指标值均是坡下高于坡上。表5参9。  相似文献   

18.
Bambooisoneofimportantreproduciblefast-growingforestresources.Itisattributedtoitsrapidgrowthrateandhighyield,andcanbeoflong-termutilizationwithonlyonceplantationandreasonablemanagement.Comparedwithwood,bamboohasgoodstrength,elasticityandhighstiffness.ForalongtimeitisusedasoneofimportantstructuralmaterialsinChinaandothercountriesinbamboo-producedregionsoftheworld.Intraditionalbamboostructuralutilization,thebamboologsareuseddirectly.Butasthelargevariationindiameterandcharacter,theyareusedonlyin…  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号