Enlargement of individual cellulose microfibrils in transgenic poplars overexpressing xyloglucanase
Authors:Mako Yamamoto  Tsuguyuki Saito  Akira Isogai  Manabu Kurita  Teiji Kondo  Toru Taniguchi  Rumi Kaida  Keiichi Baba  Takahisa Hayashi
Institution:(1) Graduate School of Environmental Studies, Nagoya University, Chikusa-ku, Nagoya Aichi, 464-8601, Japan;(2) Graduate School of Bioagricultural Sciences, Nagoya University, Chikusa-ku, Nagoya Aichi, 464-8601, Japan;(3) SCIVAX Co., Kawasaki 213-0012, Japan;(4) Graduate School of Environmental and Human Sciences, Meijo University, Nagoya 468-8502, Japan;(5) Research Institute, Meijo University, Tenpaku-ku, Nagoya 468-8502, Japan;(6) Wood Research Institute, Kyoto University, Gokasho Uji, 611-0011, Japan
Abstract:Holocellulose samples prepared from transgenic poplars overexpressing xyloglucanase had crystal widths of 3.2–3.5 nm as a result of the (2 0 0) plane, based on their X-ray diffraction patterns, and crystal widths were greater than those of the wild type (3.0 nm). Cellulose microfibril widths in the holocellulose samples were further determined from transmission electron microscopic (TEM) images of individualized fibrils prepared by 2,2,6,6-tetramethylpiperidine-1-oxy radical-mediated oxidation of the holocelluloses and the successive disintegration of the oxidized products in water. The TEM images also supported the finding that cellulose microfibril widths of transgenic poplars were larger than those of the wild type. The cellulose microfibril widths of transgenic poplars were approximately 6 nm, whereas those of the wild type were about 5 nm. However, such enlargement of cellulose microfibril widths could not be explained by the increased cellulose contents of the transgenic poplars alone.
Keywords:
本文献已被 SpringerLink 等数据库收录!