首页 | 本学科首页   官方微博 | 高级检索  
     


The influences of log storage and kiln drying climate on the colour of non-steamed beech (Fagus sylvatica L.) wood
Abstract:Abstract

Discolouration during the drying of non-steamed beech is a major industrial concern. The generally preferred yellow-white colour can easily develop a reddish or dull grey appearance during drying. In this study, the influences of log storage time and kiln drying climate on the colour of non-steamed sawn beech have been investigated and quantified. Samples 27×87 mm in cross section were dried in laboratory kilns and the average colour, in CIELAB colour space was measured on dry planed surfaces using a photoelectric colorimeter. Log storage for 13 weeks under low-temperature conditions had no visible effect. The reddish discolouration is mainly temperature related while the greyish discolouration is mainly controlled by the equilibrium moisture content (EMC) during the initial drying. Within the investigated climate interval, the EMC was twice as important as temperature for the final colour. Regression models developed show that, as long as the EMC is kept below 15%, a temperature of up to 37°C can be allowed without any visually detectable discolouration.
Keywords:Beech  discolouration  Fagus sylvatica  kiln drying  log storage
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号