HOUXinyi1 JIANGXiaomei1 GAOJianmin2 YINYafang1 1.Research Institute ofWood Industry,Chinese Academy of Forestry Beijing 100091,P. R. China; 2.Collegeof Wood Scienceand Technology,Beijing Forestry University Beijing 100083,P. R. China
摘 要:
1 MATERIALSAND METHODS 1.1 Materials The test specimens were made according to ASTM whose dimension was 20.0 mm×127.0 mm×1.20 m (thickness×width×length). The size and number for individual test’s smaller samples are listed in Table 1. Table 1. Smaller samples for individual test 1.2 Methods 1.2.1 Shaping A single spindle shaper was used to test shaping properties, which was equipped with a moulding- Individual test Size (T × W × L)(mm) Number Shaping 19.0×76.0×305.0 29 B…