CA-B/新型石蜡乳液复配处理材的防霉性能研究
引用本文:钟卉,王佳敏,汤少怀,马尔妮. CA-B/新型石蜡乳液复配处理材的防霉性能研究[J]. 农业科学与技术, 2014, 15(12): 2053-2056
作者姓名:钟卉  王佳敏  汤少怀  马尔妮
作者单位:北京林业大学材料科学与技术学院,北京,100083
基金项目:北京林业大学2014年北京市级大学生创新创业训练计划项目“CA/石蜡乳液复配处理材的微生物劣化性能研究”,中央高校基本科研业务费专项基金资助“木质材料保护技术与理论”(TD2011-14).Supported by Beijing Municipal Student Research Training Program in Beijing Forestry University,Fundamental Research Funds for the Central Universities in China
摘    要:[目的]该研究基于天然表面活性剂开发出了石蜡防水剂与铜唑(CA-B型)防腐剂的复配体系,考察了复配体系处理材的防霉防蓝变性能。[方法]采用0.3%和0.5%2种浓度的CA-B和0.5%、1.0%、2.0%3种浓度的石蜡乳液制备复配体系,利用满细胞法浸注处理50 mm(L)×20 mm×5 mm的南方松(Pinus spp.)试材,根据国标GB/T18261-2000针对蓝变菌可可球二孢(Botryodiplodia theobromae Pat.)和霉菌黑曲霉(Aspergillus niger V.Tiegh)、绿色木霉(Trichoderma viride Pers.ex Fr.)对复配处理材进行抗蓝变和抗霉变试验。[结果]石蜡乳液和CA-B均能改善木材的抗霉变和抗蓝变效果,但在一定范围内,石蜡乳液浓度增加对抗霉变和抗蓝变效果略有负面影响。[结论]以期促进木质生物质资源的高附加值利用,推动行业向更高效、更环保的方向发展。

关 键 词:铜唑(CA)  石蜡防水剂  复配  防霉防蓝变  木材

CA-B/New-type Paraffin Emulsion Compound System: Study on the Mould Preservation Property of Treated Wood
Hui ZHONG,Jiamin WANG,Shaohuai TANG,Erni MA. CA-B/New-type Paraffin Emulsion Compound System: Study on the Mould Preservation Property of Treated Wood[J]. Agricultural Science & Technology, 2014, 15(12): 2053-2056
Authors:Hui ZHONG  Jiamin WANG  Shaohuai TANG  Erni MA
Affiliation:( College of Materials Science and Technology, Beijing Forestry University, Beijing 100083, China)
Abstract:[Objective] The aim was to develop the compound system of paraffin emulsion and CA based on natural surfactants to improve the properties of anti- mould and anti-blue stain. [Method] The paraffin wax emulsion with different con- centrations of 0.5%, 1.0% and 2.0% was added into CA (0.3% and 0.5%) to obtain six groups of compound systems. The full-cell process was applied to treat the sapwood of Pinus spp. at size of 50 mm (L)×20 mm (R)×5 mm (T). Anti-mould and anti-blue stain tests were conducted using Botryodiplodia theobromae Pat., Spergi/lus niger V. Tiegh and Trichoderma viride Pers.ex Fr. according to the GB/T18261-200. [Result] Both paraffin wax emulsion and CA-B could prevent wood against mould and blue stain. However, within a certain range, anti-mould and anti-blue stain ef- fects of wood samples treated by the compound systems reduced slightly as the concentration of paraffin wax emulsion increased. [Conclusion] The research provides references for advancing use of wood biomass resources in a more efficient and more environment-friendly way.
Keywords:CuAz  Waterproof  Compound system  Anti-mould and anti-blue stain  Wood