首页 | 本学科首页   官方微博 | 高级检索  
     

THE STUDY FOR LARGE INCLUSIONS OF STAINLESS STEEL (1Crl8Ni9Ti) DURING CONTINUOUS CASTING
引用本文:Li Gang Wei Ruihang You Dingfang. THE STUDY FOR LARGE INCLUSIONS OF STAINLESS STEEL (1Crl8Ni9Ti) DURING CONTINUOUS CASTING[J]. 保鲜与加工, 1993, 0(2): 79-83
作者姓名:Li Gang Wei Ruihang You Dingfang
作者单位:Li Gang Wei Ruihang You Dingfang
摘    要:This paper presents the process of stainless steel ( 1Crl8Ni9Ti) in continuous casting,the components and their shapes,origins and distributions of the large inclusions existing in the steel,as well as the influence on its quality. By the observation through a microscope,the structural analysis adopting x-ray examinating instrument and the measunement for the microzone of billet employing the electronic probe.it has been found that the large inclusions of continuous billet mainly originate from the slag-sweeping of the tundisy and mold. There are mostly spherical-slag in addition to Ti(C.N) in the inclusions. The calculations in theory point out that the siO2in the slag can' t change Ti(C,N) into TiO2,however,it can assimilate with Ti(C.N). The large inclusions affect the quality of the steel plate and tube greatly. As a result,this paper proposes the measures of reducing the large inclusions in the steel.

关 键 词:continuous casting steel  stainless steels billets  /inclusions

THE STUDY FOR LARGE INCLUSIONS OF STAINLESS STEEL (1Crl8Ni9Ti) DURING CONTINUOUS CASTING
Li Gang Wei Ruihang You Dingfang. THE STUDY FOR LARGE INCLUSIONS OF STAINLESS STEEL (1Crl8Ni9Ti) DURING CONTINUOUS CASTING[J]. Storage & Process, 1993, 0(2): 79-83
Authors:Li Gang Wei Ruihang You Dingfang
Affiliation:Li Gang Wei Ruihang You Dingfang
Abstract:This paper presents the process of stainless steel ( 1Crl8Ni9Ti) in continuous casting,the components and their shapes,origins and distributions of the large inclusions existing in the steel,as well as the influence on its quality. By the observation through a microscope,the structural analysis adopting x-ray examinating instrument and the measunement for the microzone of billet employing the electronic probe.it has been found that the large inclusions of continuous billet mainly originate from the slag-sweeping of the tundisy and mold. There are mostly spherical-slag in addition to Ti(C.N) in the inclusions. The calculations in theory point out that the siO2in the slag can' t change Ti(C,N) into TiO2,however,it can assimilate with Ti(C.N). The large inclusions affect the quality of the steel plate and tube greatly. As a result,this paper proposes the measures of reducing the large inclusions in the steel.
Keywords:continuous casting steel  stainless steels billets  /inclusions