摘    要:从理论与实际结合出发,分析了管道腐蚀后的剩余强度。介绍了目前国际上普遍采用的以美国标准(ANSI/AMSEB31G)为代表的对管道剩余强度的评价方法,以及该方法在我国管道的适用情况。

关 键 词:腐蚀 时效分析 爆破 试验 输油管道

Pipeline prescription analysis after corrosion and explosive test,
Chen Jianmin and Meng Huimin et al. Pipeline prescription analysis after corrosion and explosive test,[J]. Oil & Gas Storage and Transportation, 1998, 17(3): 28-30
Authors:Chen Jianmin and Meng Huimin et al
Affiliation:Chen Jianmin and Meng Huimin et al
Abstract:The article analyzes pipeline's residual strength after corrosion proceeding from theory combining with practice, introduces an evaluating method of pipeline residual strength commonly applied internationally at present, taking American Standard (ANSI/AMSE B31 G) as representative, and an applicable condition of the method for our country's pipeline. Based on hydraulic explosive tests on different material qualities with given surface defects and different pipe diameters, and compared explosive results with theoretical calculation results in American standard, it is evident that the regulation of American Standard is applicable for our country. This will has a certain reference value to the operation and management of our pipeline.
Keywords:pipeline steel pipe   corrosion   evaluation   strength   explosion   test  