Charcoal was produced from short rotation tropical species ofLeucaena leucocephala andTectona grandis. The combustion-related properties, moisture content, specific gravity and percentage element composition of carbon, hydrogen, oxygen, nitrogen, sulphur and ash in wood and charcoal from the two species were determined. The gross heat of combustion of wood and charcoal was also determined.There were significant differences in the moisture content, specific gravity and percentage element composition between wood and charcoal from the two species. The carbon and ash content of charcoal were higher than those of wood. The average heat of combustion of charcoal 25.25 MJKg–1 was higher than that of wood 13.75 MJKg–1.  相似文献   

2.
观光木的生材性质研究   总被引:3,自引:0,他引:3  
对观光木的生材密度、含水率、树皮率及心材率进行测定分析,结果表明:观光木的生材密度从髓心向外呈先减小再增大的趋势,随着树高的增加,亦呈先减小再增大的趋势,其平均值为0.873 g.cm-3;基本密度自髓心向外逐渐增大,随着树高增加,呈先减小后增大再减小的趋势,其平均值为0.423 g.cm-3;含水率从髓心向外呈减小的趋势,随着树高的增加,呈先增大后减小再增大的趋势,其平均值为108.4%;树皮的体积百分率及质量百分率均随着树高的增加而增加,其平均值分别为13.5%、15.8%;心材率随着树高的增加而减少,心材百分率平均值为15.6%。  相似文献   

3.
To elucidate the development of heartwood,bark,sapwood,pith and specific gravity of wood in fastgrowing teak(Tectona grandis)plantations in Costa Rica,we sampled three trees in each of 55 plantations and modelled each variable with age,site and different tree heights.Age and stand density of plantations were significant correlated with stem diameter at breast height and total height of the tree.Formation of heartwood was initiated at the age of 4-year-old and increased in direct proportion with age.The age of plantation had a significant relationship with stem diameter at breast height,heartwood percentage,sapwood thickness,sapwood percentage,percentage of bark,pith diameter and percentage,and specify gravity.The model for these tree parameters was model with these parameters as dependent variable and in relation to age as independent variable.  相似文献   

4.
采用排水法、体积法及质量法对阴香树的生材密度、含水率、树皮率及心材率进行测定.结果表明:阴香的生材密度从髓心向外北向呈现先降低后增大的变化趋势,而南向则呈现逐渐降低的趋势,在树高方向生材密度变化较为波动,但基本上呈现先增大后减小的趋势,其平均值为1.210g/cm3.阴香木的基本密度从髓心出现先降低后增大的规律,在树的高度方向上表现出先减小后增大再减小的趋势,阴香木基本密度的平均值为0.548g/cm3.阴香木的生材含水率从髓心位置向外逐渐减小,测试的生材含水率平均值为122.5%.树皮体积百分率及质量百分率的变化规律是均随着树高的增加而增加,其平均值分别为13.86%和15.2%.随着树木高度的增加,心材率反而降低,其平均值为42.0%.  相似文献   

5.
Variations in carbon content in wood among 102 clones, selected from almost the entire natural distribution area, were investigated in Larix kaempferi. The average carbon content was 50.50%, 50.94%, and 50.80% in sapwood, heartwood, and whole wood, respectively. The difference in carbon content between clones was significant. The clonal repeatabilities were 0.46, 0.38, and 0.44 in heartwood, sapwood and whole wood, respectively. The coefficients of variation in the clonal mean carbon content were only 0.43%, 0.42%, and 0.41% in heartwood, sapwood, and whole wood, respectively. This small genetic variation and resulting small relative genetic gain of carbon content indicate that the genetic improvement of carbon content by selection has a small effect on the genetic improvement of carbon sequestration capacity by selection in L. kaempferi.  相似文献   

6.
The inorganic element contents of trees were measured to evaluate the safety of using wood biomass as thermal power generation fuel. Twelve species of typical conifer trees and 17 species of typical broad-leaved trees in Japan plus 9 species of commonly imported trees were selected and analyzed for the main inorganic elements and several trace elements that are potentially harmful in combustion ash. The ash content in bark, especially in the inner bark, was higher than that in wood, but the highest concentration was in the leaves. In almost all parts of the trees, the order of inorganic element concentration was calcium ≥ potassium ≥ magnesium ≥ sulfur ≥ phosphorous. Among the trace elements, the boron content was high and the mercury content was recorded as being high in conifer bark.  相似文献   

7.
Summary The purpose of this study was to examine the influence of the moisture level on the cell-wall material in wood using pulsed proton nuclear magnetic resonance. The wood species used were western hemlock (Tsuga heterophylla (Raf.) Sarg.) and sitka spruce (Picea sitchensis (Bong.) Carr.), distinguishing between heartwood and sapwood regions. The moisture contents of the specimens were below the fibre saturation point and they were conditioned to equilibrium moisture contents based on initial desorption, adsorption and secondary desorption processes. From the FID experiments, the NMR-based moisture contents and the solid-wood lineshape second moments were determined. Average relative proton-spin densities, which were needed to calculate the NMR-based moisture contents, were determined from known moisture contents and they were: hemlock sapwood: 0.616; hemlock heartwood: 0.537; spruce sapwood: 0.679; and, spruce heartwood: 0.446. The average RSD value, considering both heartwood and sapwood, for western hemlock species was 0.577 and for sitka spruce was 0.563; these are close to published RSD values for other species. The condition as to how the equilibrium moisture content was attained did not influence the second moment for hemlock; however, for spruce sapwood, the second moments were sorption dependent. The hemlock M2 decreased from about 5.1 × 109 s-2 at low MNMR to 4.5 × 109 s-2 (heartwood) and 4.3 × 109 s-2 (sapwood) at higher mnmr. The adsorption and secondary desorption M2 for the spruce sapwood region decreased from about 5.0 × 109 s-2 at low mnmr to about 4.1 × 109 s-2 near the MF, whereas M2 for the spruce heartwood decreased from about 4.3 × 109 s-2 at low MNMR to about 3.5 × 109 s-2 near MF. Extractives may have a key role in obtaining the RSD and second moments.This project was financially supported by the Science Council of British Columbia, MacMillan Bloedel Research. The Natural Sciences and Engineering Research Council of Canada is acknowledged for their support of the NMR spectrometer measurements  相似文献   

8.

Context

Information about variations in basic density (BD) and carbon content (%C) along tree stems is key to assessing forest carbon sinks.

Aims

The aim of the study was to determine any differences in %C and BD between different woody tissues (bark, sapwood and heartwood) in two widespread European oak species (Quercus pyrenaica and Quercus petraea).

Methods

Twenty trees were felled in northern Spain, and 317 discs cut from the trees were dried and analysed to determine %C and BD.

Results

There were significant differences in %C between bark, heartwood and sapwood, and between species. There were also significant differences in BD between the tissues (heartwood?>?sapwood?>?bark), and the BD was higher in Q. petraea than in Q. pyrenaica. Both %C and BD varied along the stem.

Conclusion

More accurate estimates of carbon contents were obtained by using specific values for different heights and anatomical parts, than by using single values.  相似文献   

9.
Heartwood, sapwood and bark content of teak trees grown in Karnataka, India   总被引:1,自引:0,他引:1  
We evaluated heartwood, sapwood and bark content in teak trees. A total of 27 sample plots were laid out in teak plantations raised by State Forest Department in Karnataka covering different age groups...  相似文献   

10.
ABSTRACT

This paper describes the chemical composition of sapwood (SW) and heartwood (HW) of Pinus halepensis Mill stem. Extractives were first isolated by accelerated solvent extraction and then analysed by gas chromatography-mass spectrometry (GC-MS). The cellulosic polysaccharide content present in the pre-extracted wood samples was determined with acid hydrolysis and GC. The hemicelluloses content was determined with acid methanolysis and GC. Free monomers were additionally analysed by GC. The amount of lignin was determined gravimetrically by the Klason lignin method and the acid-soluble lignin was determined by a UV method. Formic and acetic acids in wood were determined after alkaline hydrolysis and analysed by HP-SEC. It was found that lipophilic and hydrophilic extractives were more abundant in heartwood (1.6% and 2.5%) than in sapwood (1.1% and 1.8%). Celluloses content was higher in sapwood (42.5%) than in heartwood (39.7%), whereas lignin, hemicelluloses and sugar monomer contents were more abundant in heartwood (28.9%, 26.8% and 0.3%) than in sapwood (28.0%, 24.5% and 0.2%). The variation in acetic and formic acids and ash contents between sapwood (0.7%, 0.2% and 0.5%) and heartwood (0.6%, 0.1% and 0.4%) was small. The acetylation degrees were found to be slightly similar in sapwood (0.4) and heartwood (0.3).  相似文献   

11.
Inter-clonal, intra-clonal and within tree variations in specific gravity and wood anatomical properties of 8-year-old grown ramets of Dalbergia sissoo Roxb. have been investigated. Radial and location-wise intra-clonal variations were non-significant for anatomical properties and specific gravity for all six clones at all three sites. However, inter-clonal variations in wood anatomical properties and specific gravity were significantly different. Inter-clonal variations in anatomical properties and specific gravity were also significant due to sites, which indicated that site-characteristics overshadowed the genetic priority of different clones for wood anatomical properties. Average fiber-characteristics of all clones showed the best performance at Lalkuan, Haldwani (site III), while average specific gravity performed well at Brandis Road, Dehradun (site I) followed by site III (Lalkuan, Haldwani) and site II (Lachchiwala, Dehradun). Within tree variations in anatomical properties like fiber length, fiber diameter, wall thickness, vessel member length and vessel member diameter due to vertical or radial direction and location (pith to periphery) are non-significant. Radial direction, location and height showed no impact on wood element variation. It indicated that there is no impact of juvenile wood, sapwood and heartwood ratio, and reaction wood on wood anatomical properties of 8-year-old ramet of D. sissoo. It further indicated that clone raised ramet of 8-year-old D. sissoo showed the characteristics of mature wood. Within tree variations in specific gravity were significant due to height, which may be related to differential sapwood and heartwood ratio in the vertical direction. Different wood elements viz. fiber length, fiber diameter, wall thickness, vessel member length and vessel member diameter showed significant correlations with each other and with specific gravity.  相似文献   

12.
对海南岛乐东尖峰岭27年生柚木6个种源的生长及与材质有关特性进行测定与分析,结果表明:种源间树皮厚度、心材宽度、基本密度差异极显著,树高、材积、枝下高、边材宽度差异显著,而胸径、边材年轮数及心材率差异不显著,说明在种源水平上对柚木进行生长和与材质有关特性的改良具有较大的潜力,尤其进行木材生长性状、基本密度和心材宽度的种...  相似文献   

13.
The heartwood of the Japanese persimmon tree (Diospyros kaki) becomes black on rare occasions and has been highly esteemed as a substitute for ebony. We attempted to clarify how the physical, mechanical, chemical, and biodegradation properties differ between sapwood and blackened heartwood. The specific gravity, equilibrium moisture content, modulus of rupture, and modulus of elasticity in the blackened heartwood were higher, and the loss tangent was lower, than those in sapwood. Furthermore, the blackened portion was more resistant to fungal and termite attacks. A section of heartwood was dark-brown, and the specific gravity and mechanical properties of this portion were slightly lower than those in sapwood. The dark-brown portion was speculated to be a sign or interrupted state of fungal attack. The blackening substance was bound tightly to cell wall components and could not be extracted with any of the organic solvents used. The findings of trace element analysis using inductively coupled plasma-mass spectrometry showed that the boron content was markedly high in the blackened portion. The findings obtained here suggest a role of boron in the antifungal properties and the blackening phenomenon of Japanese persimmon.Part of this work was presented at the 50th Annual Meeting of the Japan Wood Research Society, Kyoto, April 2000  相似文献   

14.
Abstract

The heartwood and sapwood from Scots pine (PS), Norway spruce (PA), and Oriental spruce (PO) were tested for susceptibility to discoloring fungi and water uptake. In addition, annual ring width and density were measured. The methods used were Mycologg for testing growth of fungi and a modified version of EN 927-5 to investigate water uptake. For pine, the heartwood showed a lower water uptake and no discoloring fungi growing in the tests. The heartwood had a significantly higher density and smaller annual ring width than the sapwood. In PA the heartwood had significantly lower discoloration than sapwood. The total water uptake in g/m2 was significantly higher in sapwood, but not the calculated moisture content. As for wood properties, the density was significantly higher in sapwood compared to heartwood, although there were no differences in annual ring width. Regarding PO, differences in water uptake could be seen between sapwood and heartwood although the densities were similar. These results show that susceptibility to discoloring fungi and water uptake is hard to correlate to a single inherent property when looking at different wood species.  相似文献   

15.
Abstract

Wood is susceptible to decay by rot fungi if it is exposed to high-moisture contents during long periods of time and it is therefore important to limit the duration of such periods. Critical points in outdoor wood structures are, for example, end grain surfaces in joints where water can get trapped after a rain. It is therefore of interest to study both absorption and redistribution of moisture in wood. This paper presents moisture content profiles during end grain water absorption and redistribution in Norway spruce (Picea abies (L.) Karst.) measured by computed tomography with the specimens in individual climate boxes. Heartwood and sapwood of two provenances (slow-grown and fast-grown wood) were included. No major differences were seen between the water uptake of the slow-grown and the fast-grown wood since the densities were similar despite of the large difference in growth ring width. However, for the sapwood specimens, the moisture content was higher further into the specimens than for the heartwood specimens in agreement with previous studies. For the slow-grown wood, the redistribution was also generally more rapid for the sapwood specimens than for the heartwood specimens.  相似文献   

16.
木材纵向气体渗透性研究   总被引:2,自引:1,他引:1  
测试了泡桐、马尾松的渗透性 ,就木材的树种、心边材、含水率对渗透性的影响进行了初步的分析。  相似文献   

17.
Five Japanese timbers, four timbers from the USA, and one Malaysian timber were evaluated for their resistance to the invasive dry-wood termite Incisitermes minor (Hagen) using laboratory choice and no-choice feeding tests with holed specimens. The highest survival rates of I. minor in both the heartwood and sapwood no-choice feeding tests were more than 70% after 3 months. When offered sapwood and heartwood choice feeding tests and the combined choice feeding tests, the highest survival rates of I. minor were more than 75% after 3 months. With regards to the percentage of wood mass losses in the no-choice and choice feeding tests, karamatsu (Larix leptolepsis), buna (Fagus crenata), and Douglas fir (Pseudotsuga menziesii) were classified as “resistant” species among the ten sapwood specimens. In the heartwood no-choice and choice feeding tests, the resistant species were buna, karamatsu, Douglas fir, sugi (Cryptomeria japonica), akamatsu (Pinus densiflora), and western red cedar (Thuja plicata). The ranking of the resistance of the ten commercial timbers against I. minor was buna > karamatsu > sugi > western red cedar > Douglas fir > rubber > western hemlock > hinoki > spruce.  相似文献   

18.
A combined effect of steaming and heat treatment was imposed on green Turkey oak wood, both for sapwood and heartwood. Steaming was carried out in an autoclave at 100–120–130°C whereas heating was carried out in an oven for 2?h at 120–180°C. Equilibrium moisture content at dry, intermediate and moist state both in desorption and adsorption, swelling, cup, twist, color change, and spectral reflectance measures were registered. Swelling and water absorption decreased due to the hydro-thermal treatment. During adsorption, heartwood showed a higher hygroscopic inertia compared to sapwood and this difference increased with temperature. Cup increased with temperature in the steaming process. Twist seemed to be affected more by quality of original trunks than treatments. The wood color was more sensitive at a steaming temperature of 130°C combined with heat treatment at 180°C. Transitional treatments assured more reliable results on homogenization of hue between sapwood and heartwood.  相似文献   

19.
为研究大径级大花序桉人工林的基本木材性质,采用排水法对35年生大花序桉人工林木材的生材密度、基本密度、树皮率、心材率以及生材含水率等指标进行了测试。结果表明:35年生大花序桉的树皮体积百分率为8.92%,树皮质量百分率为12.35%,生材密度为1.12g·cm^-3,基本密度为0.76g·cm^-3,生材含水率为44.79%。各部位含水率差别不大,各指标表现都很好。  相似文献   

20.
Heartwood, sapwood, and inner and outer bark of Port Orford cedar were extracted with methanol, and the extracts evaluated for antioxidant activity. The total phenol content (TPC) of the extracts was determined by the Folin-Ciocalteu method and expressed as gallic acid equivalent (GAE). Butylated hydroxytoluene was used as a positive control in the free-radical-scavenging activity tests and ethylenediaminetetraacetic acid dihydrate disodium salt served as a positive control in the metal-chelating activity assay. All wood extracts showed significant freeradical-scavenging activity. In the radical-scavenging assay of 2,2-azino-bis (3-ethylbenzothiazoline-6-sulfonic acid) diammonium salt (the ABTS assay), the inner bark extracts exhibited the strongest free-radical-scavenging activity. The 50% inhibitory concentrations (IC50) in the radical-scavenging assay against 1,1-diphenyl-2-picrylhydrazyl hydrate radical (DPPH) of the heartwood, sapwood, and inner and outer bark extracts were 64.77, 29.03, 10.31, 19.87 μg·ml−1, respectively. In the metal-chelating activity system, the sapwood extract demonstrated significant activity. The greatest TPC, 537.5 mg GAE/g dry extract, was detected in the inner bark. The lowest TPC of 136.9 mg GAE/g dry extract was observed in the heartwood dry extract. The results indicate that the antioxidant activities of the extracts are in accordance with the amounts of phenolics present; the inner and outer barks of Port Orford cedar are rich in phenolics and may provide good sources of antioxidants.  相似文献   