1.
为考察打浆过程中添加羧甲基纤维素钠(CMC-Na)对杨木碱性过氧化氢化学机械浆(APMP浆)悬浮液屈服应力的影响,在分析杨木APMP浆打浆度与屈服应力关系的基础上,先添加一定量的CMC-Na对杨木APMP浆进行预处理10 min后,再分别用瓦利打浆机和PFI磨打浆处理,分析不同打浆方式以及添加CMC-Na预处理后对杨木APMP浆的打浆度和屈服应力的影响。结果表明:对于相同打浆度的杨木APMP浆,屈服应力(τ_y)随着浆料质量分数(C_m)的增加而迅速增加,且符合指数方程τ_y=aC_m~b,其中a与b值与打浆方式和打浆度的大小密切相关;经低浓度游离状的瓦利打浆机处理的浆料,其屈服应力随着打浆度的增加而减小,而中高浓度黏状的PFI磨打浆处理结果则相反。打浆过程预添加CMC-Na时,浆料打浆度随CMC-Na添加量(以绝干浆质量计)的增加先升高后降低;当CMC-Na添加量为2%并预处理10 min时,经瓦利打浆机处理的浆料打浆度可由45°SR提高到48°SR,而经PFI磨处理的浆料打浆度可由40°SR提高到50°SR,并且浆料悬浮液的屈服应力均达到最低值,分别为16.4和22.8 Pa(浆料质量分数为3%)。  相似文献   

2.
酶处理对混合杨木P-RC APMP浆打浆性能的影响   总被引:1,自引:0,他引:1  
探讨了纤维素酶、木聚糖酶处理对混合杨木温和预处理和盘磨化学处理的碱性过氧化氢机械浆(P-RC APMP)的打浆性能和打浆能耗的影响。结果表明:与未经过酶处理浆相比,纤维素酶和木聚糖酶处理可明显改善纸浆的打浆性能和降低打浆能耗,纸浆打浆度提高1.0~6.5°SR,或在相同打浆度下打浆能耗降低10%~25%。纤维素酶处理浆裂断长提高18%,撕裂指数提高14%,耐破指数提高16%,耐折度提高100%。木聚糖酶处理纸浆白度提高1.7度(ISO),纸浆物理强度略有上升。纤维素酶在改善纸浆打浆性能、降低打浆能耗和提高物理强度方面好于木聚糖酶,木聚糖酶在改善纸浆光学性能方面优于纤维素酶。酶处理可以使纸浆纤维结构变得疏松柔软,从而增强纤维间的交织能力。  相似文献   

3.
为研究稻草氧碱浆的打浆特性,采用PFI磨考察了不同打浆度对稻草氧碱浆滤水性能、纤维形态的影响,并分析其纸张强度性能的变化。结果表明:纸浆打浆度与保水值在打浆初期快速上升,在打浆后期上升趋缓,但是打浆度在打浆初期能快速上升至55~60°SR,而保水值快速上升阶段仅到45°SR左右;同时杂细胞的存在对滤水性能不利。打浆度35~75°SR过程中,纤维长度的变化不大,未除杂浆纤维长度下降最多约为7.3%,除杂浆纤维长度下降最多约为4.0%,而打浆对纤维表面的细纤维化作用明显。未除杂浆纸张耐破指数和抗张指数在打浆度65°SR时达到最佳,杂细胞的存在会对纸张的抗张强度提高形成一定的阻碍,除杂浆纸张耐破指数和抗张指数在65°SR以上的高打浆度下仍然保持上升的趋势,因而更倾向于在高打浆度、高结合强度要求的纸种当中获得应用。  相似文献   

4.
选取市场上具有代表性的两种商品针、阔叶木浆进行PFI打浆处理,研究在不同打浆度下浆料纤维质量、动态滤水性能、Zeta电位、微观结构等方面的变化,并对不同比例配抄条件下的成纸性能进行考察,结果表明:针、阔叶浆的打浆度与打浆转数之间的关系均符合线性分布:y=17.7503+0.0015x,R^2=0.9914(针叶浆);y=8.8986+0.00275x,R^2=0.9734(阔叶浆);经PFI打浆后,两种木浆纤维长度、宽度变化较小,细小组分含量变化明显;随着打浆度的升高,两者的滤水性能下降,Zeta电位先上升然后基本保持不变;初始打浆度下,随着针叶浆比例的减少、阔叶浆比例的增加,成纸的抗张强度先下降再增大,厚度逐渐下降至不变,定量逐渐增加,柔软度逐渐下降;随着打浆度的升高,成纸的抗张强度增大,厚度、定量逐渐下降,针叶浆成纸柔软度逐渐下降,阔叶浆成纸柔软度先升高再逐渐降低。  相似文献   

5.
对不同浓度、温度、打浆度、剪切速率对低浓杉木间伐材机械浆流变特性的影响进行了实验研究,并对不同因素引起浆料表观粘度变化的机理进行了分析。结果表明:浆料浓度、打浆度、温度及剪切速率都会对浆料的表观粘度产生影响。随着浆料浓度的增加,浆料表观粘度呈指数式增加;随温度的升高,浆料表观粘度则缓慢下降;打浆度影响浆料的微观结构,随着打浆度的升高,纸浆的表观粘度呈下降趋势;低浓纸浆的表观粘度则随剪切速率提高而递减。在实验测量范围内,杉木间伐材低浓纸浆为满足幂律关系的非牛顿流体,拟合的本构方程的流变特性指数n<1,因此其在测量范围内为假塑性流体。低浓纸浆流变特性的研究纸浆模塑生产线流送系统设计提供了依据。图12表2参16。  相似文献   

6.
以进口的针叶木浆为主要原料研究不同的打浆度、干燥条件对表层纸吸水高度的影响 ,探索了阴离子型物质和湿强剂用量对表层纸湿强度的影响。结果表明 :单独采用聚酰胺环氧氯丙烷还不能达到表层纸的质量要求 ,采用双元聚合物体系 ,分别加入 1.5 % (对绝干浆 )聚酰环氧氯丙烷和 1.3%的弱阴离子物质可大幅度改善纸张的湿强度。通过控制浆料的打浆度和抄片器的真空度可明显改善表层纸的吸收性能 ,其最佳的打浆度为 32~ 34°SR ,抄片器的真空度应控制在 10kPa。  相似文献   

7.
对稻草经氧碱蒸煮后进行疏解,研究疏解对稻草氧碱浆滤水性能的影响,并分析纤维质量、浆中灰分及硅含量的变化。结果表明:去除杂细胞后浆料的打浆度能降低近10°SR,疏解对浆料滤水性能的下降作用明显,同时疏解对纤维细胞的变形作用影响了浆料的打浆度,而杂细胞的存在与否对疏解浆料的打浆度影响不明显。与除杂浆料相比,未除杂浆料在疏解过程中细小纤维组分增加3.7个百分点,未除杂浆的扭结指数、卷曲指数、纤维宽度以及所含灰分中的硅含量随疏解而下降。  相似文献   

8.
试验主要以水解度为指标,综合考虑加酶量、底物浓度、温度以及pH值对影响因素,通过响应面法筛选碱性蛋白酶水解鲫鱼蛋白最佳工艺条件。试验结果表明加酶量(E/S)为1.5%、底物浓度为1%、温度45℃、pH值为9.5。水解度为12.31%。  相似文献   

9.
36-1CP高浓、高压盘磨机的结构特点(150822)方正林业造纸厂王乐新,仲丛岩,邵长梅36-1CP高浓、高压盘磨机是我厂从奥地利引进的磨浆设备。经过两年多的生产实践表明,该磨机生产性能稳定,纤维切断少,适合于林区造纸生产半化学浆。该机操作时,由于...  相似文献   

10.
采用超声辅助提取法从无患子果皮中提取无患子皂苷,通过单因素试验考察了乙醇浓度、提取时间、料液比以及提取次数4个因素对无患子皂苷得率的影响,并采用响应面法确定无患子皂苷的最佳提取工艺条件为:乙醇体积分数82.2%、提取时间33.75 min、料液比1:28.9、提取次数4次,在此优化条件下无患子皂苷的理论提取率可达到21.52%。依实际试验情况,将其修正为乙醇体积分数82%、提取时间34 min、料液比1:29、提取次数4次,经验证此条件下无患子皂苷提取率为21.48%,与理论值较为接近,表明采用响应面法分析优化无患子皂苷超声辅助提取工艺的方法可行。  相似文献   

11.
以尤溪县坂面镇坂面村湿加松和马尾松造林早期效果为切入点,对比分析了造林成活率、胸径、树高等指标,结果表明:4a生湿加松径生长和高生长明显快于同期的马尾松生长,在成活率上两者相差不大。  相似文献   

12.
马尾松地理起源及进化繁衍规律的探讨地   总被引:11,自引:0,他引:11       下载免费PDF全文
通过地史变迁、冰川影响、地形特点、生态条件的分析与植株原始形态的调查检测 ,提出四川盆地的马尾松种源是我国古老马尾松的原始类型。由于盆地的特殊地形 ,使马尾松渡过冰期的影响得以保存而生长到现在。经检测该地区马尾松针叶树脂道数目最少 ,只有大多数种源的一半 ,条叶型苗木比例最高 ,比大多数种源高 2  6倍。树脂道少与条叶型苗木多都是较为原始的形态特征 ,证明四川盆地种源属于原始类型 ,是马尾松地理起源种群。又由于盆地东南部与外界沟壑相连 ,植物基因交流渠道通畅 ,使得马尾松从原始分布区 ,经过渡地带不断进化繁衍到全国各地  相似文献   

13.
Both of straight and inclining poplar clone 107 tree were selected for studying materials in this paper.The optimal pulping conditions was established by orthogonal experimental design both for normal wood and tension wood,and the quality of pulping and paper-making between normal wood and tension wood was compared with each other. Finally,potential application for improving paper quality of tension wood through increasing beating revolutions was discussed.The result showed that the optimal cooking condition for normal wood was alkali concentration 15%,the highest temperature 164℃,time at highest temperature 75 min,and for tension wood it was alkali concentration 13%,the highest temperature 160℃,time at highest temperature 40 min.Path coefficient of effect of alkali concentration both on pulp yield and kappa value was significant at different levels.By comparison between average result of normal wood and tension wood in quality of pulping and paper-making,it was found that tension wood had higher pulping yield and lower kappa value than normal wood. Furthermore,for all mechanical properties of paper, normal wood hold higher value than tension wood, and even near two times than tension wood,such as burst index and tensile index.However,difference of tear index was quite narrow.Result of one way ANOVA showed that difference of burst index and tear index between normal wood and tension wood was significant at the 0.001 level,of tear index was significant at the 0.05 level.Based on observation of cross surface of paper,it was assumed that contribution of gelatinous layer to rigidity of single fiber had hampered collapse and compression of fiber during paper formation,which is essential for exerting combination between fibers in paper.So, mechanical properties of tension wood paper were decreased accordingly.However,owing to high cellulose content of gelatinous layer,tension wood was easier to pulping than normal wood.Mechanical properties of tension wood paper could be improved by increasing beating revolutions,  相似文献   

14.
对松实小卷蛾、松梢螟的为害性和空间格局及在序贯抽样技术中的应用的研究结果表明,二虫对松树为害具有选择性,松实小卷蛾幼虫主要为害侧枝,为害程度火炬松>黑松>湿地松>马尾松,松梢螟为害则以主梢为主,为害程度 黑松>湿地松>马尾松>火炬松.松实小卷蛾和松梢螟的空间格局分别为负二项分布和奈曼分布,松实小卷蛾明显超过防治指标,急待全面防治,松梢螟低于防治指标,可不防治.  相似文献   

15.
湿地松、火炬松适应性分析   总被引:1,自引:0,他引:1  
在同样的立地条件和抚育条件下,在1~20 a内,湿地松的生长明显优于火炬松和马尾松。20~30 a内,国外松生长不如马尾松,而且对地力的适应性也不如马尾松。作为短轮伐期的速生丰产纸浆林,湿地松是适应性比较强的速生丰产的引进树种,但在立地差、集约度低或海拔高处应以本地树种马尾松为主。  相似文献   

16.
对广东省19个马尾松主产区的508个优良马尾松单株,进行了多地点、多重复的选择研究。共选择出马尾松优良亲本和无性系59个。其中,根据子代生长量、花期、种子品质和木材比重四个综合指标评选出23个马尾松最优无性系。入选的最优无性系与CK相比,树高>7.6-20.2%,胸径>15.3-30.9%,材积>42-102%,千粒重>12.26%,发芽率>82.42%,木材比重>12.5%。  相似文献   

17.
马尾松毛红椿混交林生长效果和土壤肥力研究   总被引:3,自引:0,他引:3  
通过马尾松毛红椿混交林和马尾松纯林生长量和土壤肥力状况的对比研究,结果表明,马尾松毛红椿混交林中马尾松胸径、树高、单株材积和总蓄积量均高于马尾松纯林。混交林中马尾松和毛红椿的生长量呈现出马尾松毛红椿混交比例4∶1>3∶1>2∶1的规律。马尾松毛红椿混交林土壤水分物理性质和化学性质均优于马尾松纯林,营造马尾松毛红椿混交林有利于提高土壤肥力。由于毛红椿生长快于马尾松,营造混交林以带状混交为佳,且毛红椿比例宜小。  相似文献   

18.
细菌肥料促进马尾松生长效应的研究   总被引:3,自引:4,他引:3       下载免费PDF全文
马尾松(pinus massoniana Lamb.)是我国主要造林树种,产于我国南部,是亚热带东部湿润地区典型的针叶树种,广泛分布于全国的15个省区,占全国用材林面积的176%;近年来,马尾松人工林土壤立地质量退化、土壤性质恶化,病虫害时有发生,特别是在中、下等立地条件地区较为严重,引起林业工作者的普遍关注;合理施用化肥可以促进林木生长,然而,按目前林场的实际情况,大面积施用还很不现实,兼之施用化肥很容易造成环境污染,不利于土壤性质的改良。细菌肥料具有用量少、使用方便的优点,能促进林木生长、较好地改良土壤,增强林木的抗逆性,又不容易污染环境等,在未来的林业生产中,将具有广阔的应用前景[1~3].  相似文献   

19.
火力楠不同混交模式生长效应调查分析   总被引:4,自引:0,他引:4  
陈清堤 《林业调查规划》2011,36(3):73-76,80
对20 a生火力楠不同混交模式生长效应调查分析,结果表明,火力楠不同模式混交造林效果优于纯林,混交林产量比增6.2%~46.4%.火力楠作为主要树种与马尾松、杉木混交宜采用行间混交,混交比例按2∶1;火力楠作为伴生树种与杉木、马尾松混交宜采用插花式混交,混交比例按1∶3,种间关系较为协调.火力楠混交林与纯林比较,林分结构比较复杂,能充分利用光照条件,枯落物多且成分复杂,有利于改善林内小气候及土壤状况,林分结构比较稳定.  相似文献   

20.
5,10,15,and 20 year old Larix gmelini and Betula platyphylla were used aspulping raw material in the research.The examination of young L.gmelini and B.Platyphyllafibrous structures showed that the fiber length and ratio of length to width of 5 years old L.gmelini noticeably differed from that of mature L.gmelini.but that of 5 year old B.platyphyllawere nearby equal to that of mature B.platyphylla.The research results indicated that 15 yearsold B.platyphylla and 20 year old L.gmelini were best suited to pulping among the eight exper-imental raw materials;10 years old B.platyphylla and 15 year old L.gmelini were optimal tothe ratio of beating degree increment and corresponding beating time.The pulp characteristics of15 year old B.platyphylla and 20 year old L.gmelini were similar to those of mature wood,andit was feasible to consider 15 years to B.platyphylla and 20 years to L.gmelini as their rotationperiod;10 years and 15 years as their thinning cycles for the papermaking forest base.  相似文献   