首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 15 毫秒
1.
X-ray diffraction was used to study variations in the crystallinity of wood and the average thickness and length of the crystallites of cellulose as a function of the number of the year ring in Norway spruce [Picea abies (L.) Karst.]. The crystallinity increased from ring 4 to ring 10 from the pith and was constant after ring 10. The crystallinity of mature wood was about 30% ± 5%. The average thickness and average length of the crystallites were 3.2 ± 0.1nm and 28 ± 2nm, respectively; and no systematic variation of these values with the number of the year ring was observed. The mean microfibril angle decreased near the pith but was constant in the mature wood.  相似文献   

2.
The longitudinal modulus of elasticity of common yew is astonishingly low in light of its high raw density. At least this was found for specimens examined at the solid wood level and at the tissue level. However, to reveal if this low axial stiffness is also present at the cellular level, tensile tests were performed on individual yew fibers and on spruce fibers for reference. The results revealed a low stiffness and a high strain to fracture for yew when compared with spruce. This compliant behavior was ascribed to a relatively high microfibril angle of yew measured by X-ray scattering. It can be concluded that the high compliance of yew observed at higher hierarchical levels is obviously controlled by a structural feature present at the cell wall level. In future studies, the biomechanical function of this compliant behavior for the living yew tree would be of particular interest.  相似文献   

3.
Abstract

The moisture sorption and swelling of spruce specimens impregnated with linseed oil and unimpregnated controls were studied in two sorption experiments: from 0 to 55% relative humidity (RH) and from 55% RH to water saturation. Sorption isotherms were also determined using a sorption balance. The impregnated specimens had lower rates of both moisture sorption and swelling than the unimpregnated controls; however, there was no significant difference in final moisture contents. In addition, the linseed oil impregnation did not improve the dimensional stability of the wood; in most cases the specimens impregnated with linseed oil swelled more than the unimpregnated controls. For the impregnated specimens, reductions in swelling rates were in most cases seen without corresponding reductions in final swelling. The moisture sorption rate was reduced for the impregnated specimens but there were generally no reductions in equilibrium moisture content.  相似文献   

4.
Abstract

Untreated Scots pine (Pinus sylvestris) and Norway spruce (Picea abies) samples were exposed above ground in a durability test for 6 years. The samples consisted of three pieces of wood, 22×95×500 mm, screwed together; two pieces lengthwise with a third piece overlapping. Weight was measured, to calculate moisture content (MC), and samples checked regularly for cracks and fungal growth. Parameters investigated were heartwood/sapwood (pine), annual ring orientation (spruce), stand site, annual ring width and density. Stand site, annual ring width and density had no influence on MC or fungal growth for either pine or spruce. Spruce samples with vertical annual rings had fewer cracks than samples with horizontal annual rings. Pine sapwood samples had a high MC and a large amount of rot fungi, while heartwood had a lower MC and no rot. Most spruce samples were similar to pine heartwood, except from a few samples that had high MC and fungal growth. Those were all sawn from the outer part of the log. Therefore, it can be stated that spruce sawn from the inner part has almost the same properties as pine heartwood, while spruce from the outer part of the log has similar properties to pine sapwood.  相似文献   

5.
A population of Norway spruce (Picea abies (L.) Karst.) from southern Poland, named Kolonowskie 0293, exhibited a very high breeding value among 1100 European populations tested in the IUFRO 1964/1968 provenance experiment. However, the original mother stand of that population no longer exists. Owing to international cooperative efforts, a reconstituted clonal seed orchard of that population was successfully established to protect the gene pool of the Kolonowskie 0293 population.  相似文献   

6.
Natural regeneration measurements are the main silvicultural objective in overaged protective forests of the Bavarian Limestone Alps. While manifold problems with these stands, especially the impact of browsing, are widely recognised, the regeneration niches of Norway spruce (Picea abies [L.] Karst.) are insufficiently known. The purpose of this study was to determine favourable combinations of site factors for the development of spruce in small, unfenced canopy gaps, located on Aposerido-Fagetum caricetosum albae forest sites. We recorded the occurrence of spruce saplings (as dependent variable) and of six site factors (as independent variables) on 480 0.5 m2-subplots. In addition, we estimated the coverage of six acid adapted plant species to determine correlations with the humus depth. A binary logistic regression analysis was used to predict the probability of the occurrence of a spruce sapling in dependency of the different site factors. Supported by other studies, we assumed that the supply of solar radiation was adequate for the sufficient regeneration of spruce within the canopy gaps. Other site factors significantly determined the regeneration niches of spruce saplings. More spruce saplings were found near hindrances and on rough surfaces than would be expected from a random occurrence of saplings. These microsite types may have characteristics, especially protection against snow gliding that promotes spruce establishment. A calculated “hindrance index”, which accounted for the number, and the distance of surrounding hindrances might be a good specific value to describe the influence of hindrances on steep slopes. The sapling establishment decreased on thin humus layers. Our assumption for the sites was that thick organic layers might represent a good seedbed for spruce. Decayed dead wood was scarce, but was exceedingly favoured by spruce saplings. Results obtained suggest that the natural regeneration establishment of spruce on steep slopes can be successfully influenced by site factors which inhibit the influence of snow gliding. According to a “positive microsite” concept, we recommend for artificial regeneration measurements with spruce, microsites close to hindrances (e.g. stumps, downed trees) and Vaccinium myrtillus as a predictor for thick, acid humus layers.  相似文献   

7.
欧洲云杉扦插繁殖技术研究   总被引:3,自引:0,他引:3  
为了快速有效地规模化扦插繁殖欧洲云杉,满足造林、绿化用苗的需要。采用全光照自动间歇喷雾装置,用河沙做基质。在林科院甘肃小陇山沙坝的实验基地做了ABT1、NAA、IBA、GGR不同激素,ABT1不同浓度和浸泡时间,5-10 cm、10-15 cm和〉15 cm三种不同插穗长度,5 a和23 a不同采穗母株年龄的嫩枝扦插试验及200 mg.kg^-1ABT1处理1 h的不同插穗类型(嫩枝带硬枝和嫩枝)的试验,用清水处理插穗做对照(CK)。试验数据采用spss12.0进行方差分析,结果表明:不同激素处理的插穗生根率差异显著。生根率大小顺序为:ABT〉GGR〉IBA〉NAA。而IBA处理的插穗生根数,根系总长和根系效果指数均大于其它处理,根系发达。ABT1不同浓度和浸泡时间处理的插穗生根率差异达极显著水平。以100.mg kg^-1和200 mg.kg^-1浸泡30 min和2 h生根率最好。50 mg.kg^-1浸泡1 h处理的插穗生根数、根系总长、根系效果指数大。嫩枝带硬枝和嫩枝生根率差异不显著,但生根数、根系总长和根系效果指数嫩枝带硬枝〉嫩枝。〉15 cm的插穗生根率和其它指标都高。采自23a生母株的插穗没有生根。  相似文献   

8.
For the period 2003–2006, fructification of Norway spruce (Picea abies [L.] Karst.) was recorded at the Kranzberg forest site in Southern Germany by employing a crane with access to the canopy of more than 266 trees. For each tree, stem diameter and growth parameters were assessed annually as well as biomass of cones and seeds, number of seeds per cone, and proportions of empty seeds for a total of 371 trees with cone crop. Genotypes at 19 enzyme coding gene loci of 110 trees were included in the study of correlations between morphological and genetic traits. Re-scaling the observed values for a virtual pure Norway spruce stand of 1 ha, cone biomass including winged seeds (oven-dried at 38°C) varied between 706.8 kg/ha in 2006 (average value per tree was 3.6 kg) and values close to zero in 2005. Corresponding values for vegetative biomass increment of the coning trees in 2006 were 9,273.0 kg/ha and 10.8 kg/tree. A significant higher biomass investment was determined for dominant trees in terms of absolute cone mass as well as in terms of cone mass relative to vegetative biomass and fructification frequency. No trade-off effects in decreased vegetative biomass growth were found in the fructification year, compared to trees that did not grow cones. Although the dominant trees invested proportionally considerable biomass in cones, they showed no significant reduction in vegetative biomass growth. In the following year no decrease in vegetative growth was detected. Based on logistic regressions and homogeneity tests, respectively, significant genetic effect became evident with respect to the gene loci AAP-B and AAT-C concerning fructification probability in the year with maximum generative biomass investment. These and closely related loci also have been found to be indicative for growth and viability, respectively, in other species.  相似文献   

9.
The main purpose of this study was to investigate the variability of the fibril angle of tracheids in earlywood of Norway spruce (Picea abies L. Karst.). Polarization confocal microscopy was chosen and compared with the method utilizing the orientation of soft rot cavities. There was a significant correlation between the soft rot and polarization confocal microscopy methods, which showed the same trend of high fibril angles in the first part of the earlywood followed by a decrease toward the end of earlywood. This declining trend was less pronounced in annual rings containing compression wood. Moreover, large variations in fibril angle occurred between neighboring tracheids. The investigation also emphasized the differences between X-ray diffraction and microscopic methods, as the large variation seen by the latter methods is not seen by the X-ray diffraction approach because of its large area of measurement. No correlation was found between fiber morphology (i.e., average length, width, density) and the average fibril angle in the investigated annual rings.  相似文献   

10.
Important wood, pulp and fibre properties were investigated on small wood samples from two Rumanian, one German and one Norwegian provenance of Norway spruce (Picea abies) grown in Sørkedalen, Norway. Several samples were collected from inside each single tree, both in radial and transversal direction in the stem. Data were collected from a total of 59 trees, each 28 years of age. All investigated properties showed close relationship to ring number (RN) (cambium age). For basic density and fibre wall thickness (FWT), a fast decline was first observed when moving from pith to bark and a minimum value was found around RN 5–8. The declining trend was then followed by an increase. Kraft pulp yield, fibre length and fibre width (FW) also increased with RN, but the increase was most pronounced close to the pith. The pulp yield (PY) more or less stabilised outside of RN 5–6. FW showed a decrease outside of RN 10–12, but this was probably due to the remarkable simultaneous drop in ring width for the investigated trees. FW decreased, while basic density and fibre length increased with increasing height in the tree. PY and FWT were not affected by height in tree. Diameter at breast height (DBH) was the most important variable indicating differences between trees in the investigated material. Basic density, fibre length and FWT decreased, while FW increased with increasing DBH. Height to crown had a positive effect on basic density, but had no influence on any of the remaining properties. Differences between provenances were found for basic density, fibre length and FW. The analyses showed that it is possible to describe the variation inside and between trees satisfactorily for a range of important wood and fibre properties.  相似文献   

11.
The demand for quantifying the biomass of stumps and roots and the carbon stored therein is related to aspects of biodiversity, site productivity, atmospheric carbon cycling issues, and the demand for bioenergy. This, in turn, creates a need to develop high-quality tools for estimating biomass and carbon-equivalents in the ground. The objective of this study was to develop decomposition functions for quantifying the remaining dry weight of the biomass of individual stumps and their associated roots in Norway spruce (Picea abies (L.) Karst.). The negative exponential model was chosen for this purpose, combined with a chronosequence approach, involving 99 stumps and their roots from three sites in Sweden. The results showed a relative decay rate of 4.6% annually for stump and root systems. Based on this rate, the time required for the loss of 50% (t0.5) and 95% (t0.95) of the wood is 15 and 64 years, respectively. Although there are many variables that affect decomposition, residual studies indicated that the remaining biomass could be predicted fairly accurately on the basis of the independent variables stump diameter and time.  相似文献   

12.
13.
The present paper deals with C and N storage in soil and vegetation, litter fall and CO2 efflux from the soil 32–33 years after early thinning in a Norway spruce (Picea abies (L.) Karst.) stand in order to evaluate the effect of thinning regime on C sequestration. At 22 years old, the stand was reduced from 3190 to 2070, 1100 and 820 trees per hectare in four replicates. The N2070 treatment represents the recommended start density in practical forestry, while the other represent a moderate to large reduction in tree number at the present stand age. Aboveground biomass was estimated from single tree measurements of diameter and height based on allometric functions. Litter fall was collected during one and a half years and soil respiration was measured on five occasions during one summer. Ground vegetation was mapped and sampled for biomass, C and N determination. A significant decrease in aboveground tree (including stump-root system) C storage of 27% and 22% due to thinning was found in the N820 and N1100 treatments, respectively, compared to the N2070 treatment. Ground vegetation C storage was little affected by treatment, while litter fall C showed a non-significant decrease in the N820 and N1100 treatments compared to the N2070 treatment. Soil respiration was significantly lower in parts of the summer in the N2070 treatment compared to the N820 treatment. The reason for this is still unexplained since no differences in soil temperature, soil moisture or litter fall chemistry was found between the treatments. No significant treatment effects on humus and mineral soil C storage could be detected. With the present soil variability, the time period of 32 years is probably too short to detect soil C differences due to thinning. The N storage followed the same pattern as for C.  相似文献   

14.
Zusammenfassung Methoden zur Entwicklung molekularer Marker mit Hilfe der Polymerase-Kettenreaktion (PCR) werden beispielhaft an den beiden forstlichen PathogenenArmillaria spp. undH. annosum erl?utert. Unter Verwendung der aus „internal transcribed spacer“ (ITS)-DNA-Sequenzen abgeleiteten Primerpaare ARM-1/ARM-2 bzw. HET-7/HET-8 konntenArmillaria spp.- bzw.H. annosum-spezifische DNA-Abschnitte mittels PCR amplifiziert werden. Diese PCR-Diagnosemethode erlaubt einen schnellen und effizienten Frühnachweis dieser beiden forstlich relevanten Wurzel- und Stockf?uleerreger in verschiedenen Substraten bzw. Pflanzengeweben. Die genetische Variabilit?t von 20A. ostoyae-Isolaten aus verschiedenen geographischen Herkunftsgebieten wurde untersucht. Die UPGMA-Clusteranalyse der unter Verwendung von 10 Decamer-Zufallsprimern (OPA 01-10) erhaltenen „random amplified polymorphic DNAs“ (RAPDs)-Muster gruppierte die Isolate in Untergruppen mit 40–96% ?hnlichkeit, was auf eine hohe intraspezifische genetische Variation hindeutet. Die potentielle Rolle der historischen und gegenw?rtigen Ausbreitung von Fichtenpflanzen für die genetische Variation vonA. ostoyae in Europa wird diskutiert. Die aufgefundenen polymorphen DNA-Marker wurden für die Erfassung der Populationsstruktur bzw. -dynamik sowie der r?umlichen Ausbreitung vonA. ostoyae-„genets“ in ausgew?hlten Befallsgebieten genutzt. Erste Untersuchungen haben unterschiedliche Ausbreitungsstrategien vonA. ostoyae in Abh?ngigkeit von Klima-, Standort- und Immissionsfaktoren aufgezeigt.   相似文献   

15.
Timber storage is a key aspect of storm damage management. After huge storms, sprinkling storage is usually the most used conservation process but anaerobic storage in sealed silos appears as good alternative to preserve wood quality over long periods. This paper investigates the impact of long-term (57 months) storage of Norway spruce logs in anaerobic atmosphere on wood properties. Tests were performed on clear wood specimens and on lumbers to determine the modulus of elasticity (E), the static bending strength (σf) and the dynamic bending strength (K). Storage effects on impregnability and colour variation were also studied. Results show no effect of storage on E, σf and K. The naturally poor impregnability of Norway spruce is not improved by the anaerobic conditions, compared to traditional wet storage. Triangle tests reveal no discernible colour variation between logs that underwent anaerobic storage and the control sample. As a conclusion, despite a mould (Gliocladium solani) frequently observed on logs surface after the storage, the process offers ideal conservation conditions. While overall cost remains the main drawback for using anaerobic storage at large scale, the process can be recommended for high value logs, especially since it has few environmental impacts.  相似文献   

16.
ABSTRACT

An IML-RESI PD 400 drilling tool and a standard spade drill bit (IML System GmbH, Wiesloch, Germany) were used to study the combined effect of wood moisture content (MC), drill bit rotational speed and feed rate on drilling resistance (DR) and feeding force (FF). Tests were made with Norway spruce (Picea abies (L.) Karst.) conditioned in a normal climate (20°C/65% RH), at 20°C/95% RH, vacuum-pressure impregnated in water, and oven-dried. Rotational speeds and feed rates had an impact on feed rate per cutting edge for the major cutting edge of the drill bit which was used for correlation with DR and FF for various MC. Impact of MC on DR and FF depended on rotational speeds and feed rates of the drill bit. For feed rates per cutting edge less than 0.09?mm, DR was higher for water saturated (WS) specimens. Negligible differences between DR for various MC were found for feed rates per cutting edge between 0.09 and 0.15?mm. DR was higher at low MC for feed rates per cutting edge which were higher than 0.15?mm. FF extremely increased in conditioned (20°C/95% RH) and WS specimens at feed rates per cutting edge less than 0.1?mm.  相似文献   

17.
Abstract

An integrated simulation tool, formed by integrating the InnoSIM sawing simulation system with the RetroSTEM simulator, was used to convert available wood raw materials from final felling into sawn timber, allowing for calculation of the three-dimensional wood properties of individual stems (stem geometry, heartwood formation, knottiness) as well as the volume, quality and value of sawn timber in a Norway spruce stand with different thinning regimes (unthinned, normal and intensively thinned). Based on the input data of sawing patterns, the simulations indicate that there are relatively small differences (<8%) in the volume yield (m3ha?1) of sawn goods resulting from sawlogs available from final felling with different thinning practices. However, intensive thinning yielded the largest stem diameters and the greatest volumes (m3ha?1) of large-sized centre goods (thickness: 50, 63, 75 mm) of rather poor quality. Normal thinning yielded the largest volume of A-grade side boards and centre goods (m3ha?1), as well as the best total value ([euro]ha?1) of sawn timber. Differences observed in sawn timber quality distribution can contribute to even more significant variation in value yields, if pricing mechanisms of timber products change to favour higher grade timber products.  相似文献   

18.
This study investigated the effects of Ips typographus (L.) damage on initial litter quality parameters and subsequent decomposition rates of oriental spruce tree species [Picea orientalis (L.) Link]. The needle litter was collected from highly damaged, moderately damaged and control stands on two aspects (north and south) and two slope position (top and bottom) on each aspect. The litter was analyzed for initial total carbon, lignin and nutrient (nitrogen, phosphorus, potassium, calcium, magnesium and manganese) concentrations. The variability in nitrogen and calcium concentrations and ratios of C:N, lignin:N and lignin:Ca was significantly affected by the insect damaged levels. While nitrogen concentrations in needle litter increased with increasing insect damage (and consequently the ratios of C:N and lignin:N decreased), calcium concentrations decreased (and consequently the ratio of lignin:Ca increased). Aspect and slope positions explained most of the variability in carbon, lignin, phosphorus, potassium, magnesium and manganese concentrations and lignin:P ratio between all studied stands. Litter decomposition was studied in the field using the litterbag technique. The litter from highly damaged stands showed highest decomposition rates followed by moderately damaged and control stands. The mass loss rates were significantly positively correlated with initial nitrogen concentration and negatively with C:N and lignin:N ratios. The effects of microclimate resulting from canopy damage on litter decomposition was also examined at the same time using standard litter with the same litter quality parameters, but they showed no significant differences among the insect damage levels indicating that alteration of the litter quality parameters produced by I. typographus damage played a more important role than altered microclimate in controlling needle litter decomposition rates. However, changes in microclimate factors due to topography influenced decomposition rates.  相似文献   

19.
The study focused on kapok [Ceiba pentandra (L.) Gaertn.] fruit as a biomass for effective utilization. Kapok fruits were harvested just before full maturation at the campus of University of the Philippines Los Banos and in southern Vietnam. The kapok fibers are utilized locally as fiberfill in pillows, quilts, and some soft toys. Kapok fiber was isolated and analyzed microscopically, and the physicochemical properties were determined by spectroscopic methods. Some tests were done to determine the effective utilization of kapok fiber. Microscopic analysis of the higher structure of kapok fiber gave quite different results from cotton fiber, which has a significantly homogeneous hollow tube shape and is composed of cellulose (35 % dry fiber), xylan (22%), and lignin (21.5%). Kapok fiber is characterized by having a high level of acetyl groups (13.0%). Usually cell walls of plants contain about 1%–2% of acetyl groups attached to noncellulosic polysaccharides. Kapok fiber is significantly hydrophobic and does not get wet with water. Thus, the absorptivity of oil was tested. The fiber selectively absorbed significant amounts of oil (40 g/g of fiber) from an oil suspension in freshwater and seawater. It is suggested that this fiber could be used to recover oil spilled in seawater.  相似文献   

20.

Key message

Fungal infection was outlined as a potential reason for the onset of indented annual growth ring formation during the juvenile phase of hazel wood growth. Annual growth ring indentations resulted from the formation of disturbed zones which originated solely in close proximity to leaf traces.

Context

Hazel wood is an abnormal type of woody tissue that is formed as a result of exogenous stimuli that may trigger long-term responses in the cambium. Cambial responses produce anatomical alterations in the surrounding xylem tissue that can be observed as an indentation of annual growth rings. The chemical profiles of lignan hydroxymatairesinol may provide an indication of its possible role in the protection of a living tree against the spread of a fungal or microbial infection at the onset of indentation.

Aims

The objectives of this study were to reveal the anatomical differences in the altered woody tissue of Picea abies hazel wood at both the onset and the later stages of annual growth ring indentation and to determine the chemical profiles for hydroxymatairesinol upon elicitation by a fungal infection in the disturbed zones.

Methods

Light and scanning electron microscopy observations were carried out on radial, tangential, and cross sections of hazel wood zones separated from P. abies stems. Concentrations of hydroxymatairesinol were determined for both the disturbed zones and the non-indented zones using a gradient high-performance liquid chromatography.

Results

The formation of disturbed zones was accompanied by significant changes in both the direction and width of the tracheids which produced an abnormal formation of intertwined and twisted tracheids. Fungal hyphae, radial cell wall cracks, and unusually large cross-field pitting were all found in the tracheids of the disturbed zones.

Conclusion

The content of hydroxymatairesinol in the acetone extract determined from the disturbed zones was 3.4 times greater than that present in the non-disturbed tissues. By means of vascular dysfunction in the leaf traces, host trees responded to the fungal infection by plugging the lumens of conductive leaf trace tissue and filling the vascular pathway with polyphenolic compound deposits.