Reducing ring spun yarn hairiness via spinning with a contact surface |
| |
Authors: | Zhigang Xia Weilin Xu Ming Zhang Weibing Qiu Shengli Feng |
| |
Affiliation: | 3. College of Textiles, Donghua University, Shanghai, 201620, China 1. Hubei Key Laboratory for New Textile Materials and Applications, Wuhan Textile University, Wuhan, 430073, China 2. Xiangyang Jihua 3542 Textile Company Limited, Xiangyang, 441002, China
|
| |
Abstract: | In this study, spinning with a contact surface was introduced as a simple and energy-saving method to reduce spun yarn hairiness. Theoretical analysis indicated that yarn hairiness could be reduced via a sufficient long contact surface applied in other part of yarn formation zone in addition to spinning triangle. Then, a simple contact apparatus was installed on ring frame to validate the theoretical analysis. Results proved that yarn hairiness was reduced via a contact surface in the yarn formation zone. However, unevenness was deteriorated for most yarns spun with contact apparatus during the spinning, which might be due to fiber mass concentration. Most of yarns spun with contact apparatus had a lower strength than the conventional yarns. This might be because evenness deterioration to decrease yarn strength overpowered hairiness reduction to increase yarn strength for most yarns spun with a contact surface. |
| |
Keywords: | |
本文献已被 SpringerLink 等数据库收录! |
|