1.
Jute fibers have immense potential to be used as natural fillers in polymeric matrices to prepare biocomposites. In the present study jute fibers were surface treated using two methods: i) alkali (NaOH) and ii) alkali followed by silane (NaOH+Silane) separately. Effects of surface treatments on jute fibers surface were characterized using fourier transform infrared spectroscopy (FT-IR) and scanning electron microscopy (SEM) analyses. Further, the effects of surface treatments on jute fibers properties such as crystallinity index, thermal stability, and tensile properties were analyzed by X-ray diffraction method (XRD), thermo gravimetric analysis (TGA), and single fiber tensile test respectively. The effects of surface treatment of jute fibers on interphase adhesion between of poly(lactic acid) (PLA) and jute fibers were analyzed by performing single fiber pull-out test and was examined in terms of interfacial shear strength (IFSS) and critical fiber length.  相似文献   

2.
Present research investigates the mechanical properties of jute-coir fiber reinforced hybrid polypropylene (PP) composite with fiber loading variation and observes the effect of chemical treatment of fiber on property enhancement of the composites. Composites were manufactured using hot press machine at four levels of fiber loading (5, 10, 15 and 20 wt%). Fiber ratio’s were varied (jute:coir=1:1, 3:1 and 1:3) for 20 % fiber loaded composites. Both jute and coir fiber was treated using 5 % and 10 % NaOH solutions. Composites were also prepared using treated fiber with jute-coir fiber ratio of 3:1. Tensile, flexural, impact and hardness tests and Fourier transform infrared spectroscopic analysis were conducted for characterization of the composites. Tensile test of composite showed a decreasing trend of tensile strength and increasing trend of the Young’s modulus with increase in fiber loading. During flexural, impact and hardness tests, the flexural strength, flexural modulus, impact strength and hardness values were found to be increased with increase in fiber loading. All these properties enhanced with the enhancement of jute content except impact strength. 5 % NaOH treatment provided an improving trend of properties whereas, 10 % NaOH treatment showed the reverse one. The FTIR analysis of the composites indicated decrease of hemicelluloses and lignin content with alkali treatment.  相似文献   

3.
Jute fabric reinforced polypropylene composites were fabricated by compression molding technique. Fiber content in the composites was optimized at 45 % by weight of fiber by evaluating the mechanical parameters such as tensile strength, tensile modulus, bending strength, bending modulus. Surface treatment of jute fabrics was carried out by mercerizing jute fabrics with aqueous solutions of NaOH (5, 10 and 20 %) at different soaking times (30, 60 and 90 mins) and temperatures (0, 30 and 70 °C). The effect of mercerization on weight and dimension of jute fabrics was studied. Mechanical properties of mercerized jute-PP composites were measured and found highest at 20 % NaOH at 0 °C for 60 min soaking time. Thermal analytical data from thermogravimetric and differential thermal analysis showed that mercerized jute-PP composite achieved higher thermal stability compared to PP, jute fabrics and control composite. Degradation characteristics of the composites were studied in soil, water and simulated weathering conditions. Water uptake of the composites was also investigated.  相似文献   

4.
Poly(lactic acid) (PLA)/jute fiber biocomposites with: i) untreated jute fiber, ii) NaOH treated jute fiber, and iii) (NaOH+silane) treated jute fibers were prepared by melt extrusion process. Microcellular foaming of the injection molded samples was carried out by using single stage batch process. The effects of jute fiber content as well as that of matrix-fiber phase adhesion, in composites with surface treated jute fibers, on the foam microstructure were studied. Further, water absorption, thickness swelling, and biodegradation behavior of the foamed biocomposites were studied and correlated with their foam microstructures. It was observed that on increasing jute fiber content in PLA/JFU biocomposites, cell density increased from 6.5×107 to 8.1×107, while the cell size and expansion ratio decreased from 40 to 23 μm and 2.41 to 1.45, respectively. Again, on increasing the extent of the jute fiber surface treatment in the biocomposites, cell size and expansion ratio increased from 40 to 78 μm and 2.41 to 2.80 respectively. This study also revealed that the rate of biodegradation accelerated with increase in the jute fiber content in the biocomposites while the same retarded with increase in the extent of jute fiber surface treatment.  相似文献   

5.
Natural fibers are largely divided into two categories depending on their origin: plant based and animal based. Plant based natural jute fiber reinforced polypropylene (PP) matrix composites (20 wt% fiber) were fabricated by compression molding. Bending strength (BS), bending modulus (BM), tensile strength (TS), Young’s modulus (YM), and impact strength (IS) of the composites were found 44.2 MPa, 2200 MPa, 41.3 MPa, 750 MPa and 12 kJ/m2, respectively. Animal based natural B. mori silk fiber reinforced polypropylene (PP) matrix composites (20 wt% fiber) were fabricated in the same way and the mechanical properties were compared over the silk based composites. TS, YM, BS, BM, IS of silk fiber reinforced polypropylene composites were found 55.6 MPa, 760 MPa, 57.1 MPa, 3320 MPa and 17 kJ/m2 respectively. Degradation of composites in soil was measured upto twelve weeks. It was found that plant based jute fiber/PP composite losses its strength more than animal based silk fiber/PP composite for the same period of time. The comparative study makes it clear that mechanical properties of silk/PP composites are greater than those values of jute/PP composites. But jute/PP composites are more degradable than silk/PP composites i.e., silk/PP composites retain their strength for a longer period than jute/PP composites.  相似文献   

6.
Chemical treatment is an often-followed route to improve the physical and mechanical properties of natural fiber reinforced polymer matrix composites. In this study, the effect of chemical treatment on physical and mechanical properties of jute fiber reinforced polypropylene (PP) biocomposites with different fiber loading (5, 10, 15, and 20 wt%) were investigated. Before being manufactured jute fiber/PP composite, raw jute fiber was chemically treated with succinic anhydride for the chemical reaction with cellulose hydroxyl group of fiber and to increase adhesion and compatibility to the polymer matrix. Jute fiber/PP composites were fabricated using high voltage hot compression technique. Fourier Transform Infrared spectroscopy (FTIR) and Scanning Electron Microscopy (SEM) tests were employed to evaluate the morphological properties of composite. Succinic anhydride underwent a chemical reaction with raw jute fiber which was confirmed through FTIR results. SEM micrographs of the fractured surface area were taken to study the fiber/matrix interface adhesion and compatibility. Reduced fiber agglomeration and improved interfacial bonding was observed under SEM in the case of treated jute fiber/PP composites. The mechanical properties of jute/PP composite in terms of Tensile strength and Young’s modulus was found to be increased with fiber loading up to 15 wt% and decreased at 20 wt%. Conversely, flexural strength and flexural modulus increased with fiber loading up to 10 wt% and start decreasing at 15 wt%. The treated jute/PP composite samples had higher hardness (Rockwell) and lower water absorption value compared to that of the untreated ones.  相似文献   

7.
In this study, jute fabrics were modified by alkali, micro-emulsion silicon (MS) and fluorocarbon based agents (FA) in order to enhance the interfacial adhesion between the polyester matrix and the jute fiber. X-ray photoelectron spectroscopy (XPS) and contact angle measurements were used to characterize fiber surfaces. The effects of various surface treatments on the mechanical and morphological of jute/polyester composites were also studied. All surface treatments were shown to improve the tensile, flexural strengths and interlaminar shear strengths of the composites. Moreover, the maximum improvement in the mechanical properties was obtained for the FA treated jute/polyester composites. SEM micrographs of the tensile fracture surface of jute/unsaturated polyester composites also exhibited improvement of interfacial and interlaminar shear strengths by the alkali, MS and FA treatments of jute fibers.  相似文献   

8.
Low-temperature pyrolysis up to 200, 250, 300 °C was conducted in order to remove non-cellulosic compounds without damaging the structure of the cellulose in jute fibers. The chemical, morphological, and mechanical aspects of prepared low-temperature pyrolyzed jute fibers were investigated by Fourier transform infrared (FTIR) spectroscopy, the wettability test in water/dichloromethane system, moisture content measurement, X-ray diffraction (XRD) analysis, scanning electron microscope (SEM), and tensile test using universal testing machine (UTM). It was confirmed that hydrophilic compounds including absorbed water, low molecular weight compounds such as waxes, hemicellulose, and lignin were largely removed from the fibers. Increasing amounts of non-cellulosic compounds were removed as the maximum pyrolysis temperature was increased. The degree of hydrophilic nature of jute fibers were reduced by low-temperature pyrolysis and thus water absorptivity of pyrolyzed jute fibers was reduced as maximum pyrolysis temperature increased. Furthermore, XRD analysis and morphological studies by SEM indicated that the crystalline structure of native cellulose was rarely damaged after pyrolysis up to 300 °C. In case of mechanical properties, breaking tenacity and breaking strain of the fibers decreased with increasing maximum pyrolysis temperatures because flaws formed on the surface of pyrolyzed jute fibers acted as weak-links. In agreement with predictions made according to Weibull’s weakest-link theory, it was found that shortened pyrolyzed jute fibers could have higher breaking tenacities compared with raw jute fibers of the same length. In addition, the compatibility with hydrophobic matrix was investigated by the mechanical properties of polypropylene (PP) reinforced with jute fibers. Consequently, it was hypothesized that low-temperature pyrolysis could be used to process raw jute fibers for use as short fiber reinforcements in fiber-polymer systems or be a simple and effective pretreatment method for a wide range of further chemical treatments.  相似文献   

9.
Human consumption of flaxseed is increasing due to its health benefit properties and extrusion processes can enhance its nutritional quality. Extruded flaxseed meal (EFM) obtained in a pilot plant was characterized and incorporated in flour mixes and cereal-based bars to demonstrate its nutritious usefulness. Amino acid content was not affected by extrusion and, despite lysine was the limitating amino acid, the chemical score (CS) was 83 %. Thiamin and riboflavin decreased slightly as consequence of extrusion, phytic acid did not change and trypsin inhibitor activity was undetectable. Proximate composition and nutritional quality determined by biological and chemical indexes were compared among EFM, flour mixes (FM) and cereal bars (CB). They presented high protein levels (26, 20 and 17 %, respectively), good biological value (BV) (80, 79 and 65, respectively), acceptable true protein digestibility (TD) (73, 79 and 78, respectively), and high dietary fiber (33, 20.5 and 18 %, respectively). The ratio of ω6:ω3 for CB was within the WHO/FAO recommendations. These results open a new venue for the usefulsess of nutritious/healthy extruded flaxseed flours into ready-to-eat cereal-based products with improved nutritional quality.  相似文献   

10.
We investigated the surface modification of jute fiber by oxygen plasma treatments. Jute fibers were treated in different plasma reactors (radio frequency “RF” and low frequency “LF” plasma reactors) using O2 for different plasma powers to increase the interface adhesion between jute fiber and polyester matrix. The influence of various plasma reactors on mechanical properties of jute fiber-reinforced polyester composites was reported. Tensile, flexure, short beam shear tests were used to determine the mechanical properties of the composites. The interlaminar shear strength increased from 11.5 MPa for the untreated jute fiber/polyester composite to 19.8 and 26.3 MPa for LF and RF oxygen plasma treated jute fiber/polyester composites, respectively. O2 plasma treatment also improved the tensile and flexural strengths of jute fiber/ polyester composites for both plasma systems. It is clear that O2 plasma treatment of jute fibers by using RF plasma system instead of using LF plasma system brings about greater improvement on the mechanical properties of jute/polyester composites.  相似文献   

11.
This research work was concerned with the evaluation of the effect of fibre content on the mechanical properties of composites. Composites were fabricated using jute/phenol formaldehyde (PF), rockwool/PF, and jute/rockwool hybrid PF with varying fibre loadings. Jute and rockwool fibre reinforced PF composites were fabricated with varying fibre loadings (16, 25, 34, 42, 50, and 60 vol.%). The jute/rockwool hybrid PF composites were manufactured at various ratios of jute/rockwool fibres such as 1:0, 0.92:0.08, 0.82:0.18, 0.70:0.30, 0.54:0.46, 0.28:0.72, and 0:1. Total fibre content of the hybrid composites was 42 vol.%. The results showed that tensile strength of the composite increased with increasing fibre content up to 42 vol.% over which it decreased for jute and rockwool fibre reinforced PF composites. Flexural strength of the composite was noted to peak at a fibre loading of 42 vol.% for jute/PF composites, and 34 vol.% for rockwool/PF composites. Impact strength of jute/PF composites increased with increasing fibre loading but that of rockwool/PF composites decreased at higher (>34 vol.%) fibre loadings. Tensile, flexural, and impact strengths of jute/PF composites were found to be higher than those of rockwool/PF composites. The maximum hardness values were obtained 42 vol.% for jute/PF composite, and 34 vol.% for rockwool/PF composite. Further increase in fibre loading adversely affected the hardness of both composites. For jute/rockwool hybrid PF composites, tensile and impact strengths decreased with increasing rockwool fibre loading. The maximum flexural strength of jute/rockwool hybrid PF composites was obtained at a 0.82:0.18 jute/rockwool fibre ratio while maximum hardness was observed at a 0.28:0.72 jute/rockwool fibre ratio. The fractured surfaces of the composites were analysed using scanning electron microscope in order to have an insight into the failure mechanism and fibre/matrix interface adhesion.  相似文献   

12.
本文针对黄/红麻的引种、育种所取得的成效,研究了黄/红麻在纺织领域应用的目的和意义,介绍了黄/红麻纤维的种类、主要产地、技术参数和分等要求,提出了黄/红麻在服用、装饰用及产业用纺织品上的应用前景。黄/红麻作为重要的天然纺织原料,必将得到充分的应用。  相似文献   

13.
The surface topography, tensile properties, and thermal properties of ramie fibers were investigated as reinforcement for fully biodegradable and environmental-friendly ‘green’ composites. SEM micrographs of a longitudinal and cross-sectional view of a single ramie fiber showed a fibrillar structure and rough surface with irregular cross-section, which is considered to provide good interfacial adhesion with polymer resin in composites. An average tensile strength, Young’s modulus, and fracture strain of ramie fibers were measured to be 627 MPa, 31.8 GPa, and 2.7 %, respectively. The specific tensile properties of the ramie fiber calculated per unit density were found to be comparable to those of E-glass fibers. Ramie fibers exhibited good thermal stability after aging up to 160°C with no decrease in tensile strength or Young’s modulus. However, at temperatures higher than 160°C the tensile strength decreased significantly and its fracture behavior was also affected. The moisture content of the ramie fiber was 9.9%. These properties make ramie fibers suitable as reinforcement for ‘green’ composites. Also, the green composites can be fabricated at temperatures up to 160°C without reducing the fiber properties.  相似文献   

14.
This study developed a novel PHB-lignin-jute biodegradable composite with preferable mechanical properties and low water absorption. The appearances of fracture surface of composites were analyzed by scanning electron microscope. The result suggested a Gaussian-like distribution of the size particles supporting the presence of lignin with a radius smaller than 0.5 μm. According to X-ray diffraction, the presence of lignin and jute fibers was decreased the crystallization of PHB. Moreover, the glass transition temperature of PHB increased, and the endotherm during glass transition was decreased. The maximum tensile strength and modulus of composites were obtained with 30 wt% jute fiber contents and 4 wt% lignin contents. The presence of jute fibers was largely increased the water absorption of composites. However, the presence of lignin was effectively decreased the water absorption of composites at saturation levels.  相似文献   

15.
Optimizing the alkali treatment process alone without tracking the changes of algae and agar quality with each pretreatment process will not achieve the optimal agar yield and final quality. In this study, we monitored the changes of the morphology and weight of algae with each treatment process, and comprehensively analyzed the effects of each pretreatment process on the quality of agar by combining the changes of the physicochemical properties of agar. In conventional alkali-extraction technology, alkali treatment (7%, w/v) alone significantly reduced the weight of algae (52%), but hindered the dissolution of algae, resulting in a lower yield (4%). Acidification could solve the problem of algal hardening after alkali treatment to improve the yield (12%). In enzymatic extraction technology, agar with high purity cannot be obtained by enzyme treatment alone, but low gel strength (405 g/cm2) and high sulfate content (3.4%) can be obtained by subsequent acidification and bleaching. In enzyme-assisted extraction technology, enzyme damage to the surface fiber of algae promoted the penetration of low-concentration alkali (3%, w/v), which ensured a high desulfurization efficiency and a low gel degradation rate, thus improving yield (24.7%) and gel strength (706 g/cm2), which has the potential to replace the traditional alkali-extraction technology.  相似文献   

16.
The increasing demand for high-fiber products has favored the design of numerous bakery products rich in fiber such as bread, cookies, and cakes. The objective of this study was to evaluate the dietary fiber and estimated glycemic index of cookies containing extruded wheat bran. Wheat bran was subjected to extrusion process under three temperature profiles: TP1;(60, 75, 85 and 100 °C), TP2;(60, 80, 100 and 120 °C), and TP3;(60, 80, 110 and 140 °C) and three moisture contents: (15, 23, and 31 %). Cookies were elaborated using extruded wheat bran (30 %), separated into two fractions (coarse and fine). The dietary fiber content of cookies elaborated with extruded wheat bran was higher than the controls; C0 (100 % wheat flour) and C1 (30 % of no extruded bran coarse fraction) and C2 (30 % of no extruded bran fine fraction). The higher values of dietary fiber were observed on cookies from treatments 5 (TP1, 31 % moisture content and coarse fraction) and 11 (TP2, 31 % moisture content and coarse fraction). The estimated glycemic index of cookies ranged from 68.54 to 80.16. The dietary fiber content of cookies was increased and the lowest glycemic index corresponded to the cookies elaborated with extruded wheat bran. Cookie made with the treatment 11 had a better dietary fiber content and lower estimated glycemic index.  相似文献   

17.
The effects of chemical treatment on the flexural and impact properties of sugar palm fiber reinforced high impact polystyrene (HIPS) composites were studied. Two types of concentration of alkali solution (4 % and 6 %) and also two types of percentage of compatibilizing agent (2 % and 3 %) have been used in this study. The alkaline treatment is carried out by immersing the fibers in 4 % and 6 % of alkali solution for 1 hour. A 40 wt. % of alkali treated sugar palm fiber (SPF) was blended with HIPS using Brabender machine at temperature of 165 °C. The second treatment was employed by compounding mixture of sugar palm fibers and HIPS with 2 and 3 % of compatibilizing agent using the same procedure. The composites plate with dimensions of 150×150×3 mm was produced by using the hot press machine. The flexural strength, flexural modulus and impact strength of composites were measured and the values were compared to the untreated composites. Improvement of the mechanical properties of the composites has been shown successfully. Alkali treatment using 6 % NaOH solution improve the flexural strength, flexural modulus and impact strength of the composites as amount 12 %, 19 % and 34 % respectively, whereas compatibilizing agent treatment only showed the improvement on the impact strength, i.e. 6 % and 16 % improvement for 2 % and 3 % MAH respectively.  相似文献   

18.
Multi-functional comonomer from pentaerythritol (PE) and terephthaloyl chloride (TPC) was synthesized and used for polymerization of poly(p-phenylene benzobisoxazole) (PBO) copolymer. PBO copolymer fibers were prepared from PBO copolymers using a dry-jet wet spinning. The tensile strength of PBO copolymer fibers was higher than that of PBO, and showed 42 % increase at 0.5 mol% loading of comonomer. The tensile modulus of PBO copolymer fiber at 0.5 mol% loading showed 192 % increase compared to PBO fiber. The compressive strength of PBO copolymer fiber had values between 0.46 GPa and 0.6 GPa with the comonomer content. 64-114 % increase in compressive strength of PBO copolymer fibers was observed compared to PBO fiber.  相似文献   

19.
The compressive and flexural properties of hemp fiber reinforced concretes (FRC) were examined in this paper. Natural hemp fiber was mixed using dry and wet mixing methods to fabricate the FRC. Mechanical properties of the FRC were investigated. The main factors affecting compressive and flexural properties of the FRC materials were evaluated with an orthogonal test design. Fiber content by weight has the largest effect. The method for casting hemp FRC has been optimised. Under the optimum conditions, compressive strength increased by 4 %, flexural strength increased by 9 %, flexural toughness increased by 144 %, and flexural toughness index increased by 214 %.  相似文献   

20.
The aim of the work was to study the influence of particle size in the composition, physicochemical, techno-functional and physio-functional properties of two flours obtained from persimmon (Diospyros kaki Trumb. cvs. ‘Rojo Brillante’ (RBF) and ‘Triump’ (THF) coproducts. The cultivar (RBF and THF) and particle size significantly affected all parameters under study, although depending on the evaluated property, only one of these effects predominated. Carbohydrates (38.07–46.98 g/100 g) and total dietary fiber (32.07–43.57 g/100 g) were the main components in both flours (RBF and THF). Furthermore, insoluble dietary fiber represented more than 68% of total dietary fiber content. All color properties studied were influenced by cultivar and particle size. For both cultivars, the lower particle size, the higher lightness and hue values. RBF flours showed high values for emulsifying activity (69.33–74.00 mL/mL), while THF presented high values for water holding capacity (WHC: 9.47–12.19 g water/g sample). The bile holding capacity (BHC) and fat/oil binding values were, in general, higher in RBF (19.61–12.19 g bile/g sample and 11.98–9.07, respectively) than THF (16.12–12.40 g bile/g sample and 9.78–7.96, respectively). The effect of particle size was really evident in both WHC and BHC. Due to their dietary fiber content, techno-functional and physio-functional properties, persimmon flours seem to have a good profile to be used as potential functional ingredient.  相似文献   